2507 zanglamaydigan po'lat quvur
1. Standart: ASTM A789, ASME SA789, ASTM A790, ASME SA790
2. OD: 1/2″ - 36″ (13,7 mm - 914,4 mm)
3. Qalinligi: 0.3 mm - 50 mm
4. Oxiri: tekis uchi, qirrali uchi, oyoq osti
5. Baholar: 2507, UNS S32750, WNR.1.4410
2507 zanglamaydigan po'lat quvur tez-tez ishlatiladigan super dupleks zanglamaydigan po'latdir. Qotishma 2507 tarkibida 25% xrom, 4% molibden va 7% nikel mavjud. Molibden, xrom va azotning yuqori miqdori xlorid chuqurligi va yoriqlar korroziyasiga mukammal qarshilik ko'rsatadi. Dupleks tuzilishi, shuningdek, xlorid stressli korroziyaga qarshi 2507 mukammal qarshilik ko'rsatadi. Dupleks s32750 600 daraja F (316 daraja C) gacha bo'lgan dastur haroratiga ega. Neft va gaz, dengiz muhandisligi va boshqalar uchun javob beradi.
ASTM A790 UNS S32750 quvurlarining qo'llanilishi quyidagilardan iborat:
- Kimyoviy texnologik sanoat tarmoqlari
- Issiqlik almashtirgichlar, idishlar va quvurlar
- Tuzsizlantirish zavodlari va boshqa sho'r suvlarni qo'llash
- Energiya sanoati FGD tizimlari
- Yong'inga qarshi tizimlarni o'z ichiga olgan offshor platformalar

Super Duplex 2507 quvurining texnik xususiyatlari
| Texnik xususiyatlari | ASTM A790, ASME SA790 |
| ASTM A789, ASME SA789 | |
| Standartlar | ASTM, ASME va API |
| Tashqi diametri | 1/2″ - 36″ (13,7 mm - 914,4 mm) |
| Devor qalinligi | 0.3 mm - 50 mm |
| Jadval | SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS |
| Uzunlik | Yagona tasodifiy, ikki marta tasodifiy, kesish uzunligi |
| Oxiri | To‘g‘ri uchi, qirrali uchi, pog‘onali |
| O'lchovli spetsifikatsiya | ANSI/ ASME B36.10, B36.19 |
| Turi | Choksiz, ERW, payvandlangan, ishlab chiqarilgan |
| Shakl | Dumaloq quvurlar, kvadrat quvurlar, to'rtburchaklar, "U" shakli, gidravlik quvurlar |
2507 zanglamaydigan po'lat quvurMexanik xususiyatlar
|
Hosildorlik kuchi: |
80 ksi min |
|
Mustahkamlik chegarasi |
116 ksi min |
|
Uzayish (min 2") |
15% |
|
Qattiqlik (Rokvell C shkalasi) |
32 HRC maksimal |
2507 Super Duplex SS quvurlari jadvali va devor qalinligi
| NPS ichida. | OD mm. | Sh | WT mm. | kg/m |
| 1/4 | 13.72 | 10S | 1.65 | 0.5 |
| 1/4 | 13.72 | 40S | 2.24 | 0.64 |
| 1/4 | 13.72 | 80S | 3.02 | 0.81 |
| 3/8 | 17.15 | 10S | 1.65 | 0.64 |
| 3/8 | 17.15 | 40S | 2.31 | 0.86 |
| 3/8 | 17.15 | 80S | 3.2 | 1.12 |
| 1/2 | 21.34 | 10S | 2.11 | 1.02 |
| 1/2 | 21.34 | 40S | 2.77 | 1.29 |
| 1/2 | 21.34 | 80S | 3.73 | 1.65 |
| 3/4 | 26.67 | 10S | 2.11 | 1.3 |
| 3/4 | 26.67 | 40S | 2.87 | 1.71 |
| 3/4 | 26.67 | 80S | 3.91 | 2.23 |
| 1 | 33.4 | 10S | 2.77 | 2.13 |
| 1 | 33.4 | 40S | 3.38 | 2.54 |
| 1 | 33.4 | 80S | 4.55 | 3.29 |
| 1 | 33.4 | 160S | 6.352) | 4.3 |
| 1¼ | 42.16 | 10S | 2.77 | 2.73 |
| 1¼ | 42.16 | 40S | 3.56 | 3.44 |
| 1¼ | 42.16 | 80S | 4.85 | 4.53 |
| 1¼ | 42.16 | 160S | 6.352) | 5.69 |
| 1½ | 48.26 | 10S | 2.77 | 3.16 |
| 1½ | 48.26 | 40S | 3.68 | 4.11 |
| 1½ | 48.26 | 80S | 5.08 | 5.49 |
| 2 | 60.33 | 10S | 2.77 | 3.99 |
| 2 | 60.33 | 40S | 3.91 | 5.52 |
| 2 | 60.33 | 80S | 5.54 | 7.6 |
| 2 | 60.33 | 160S | 8.742) | 11.29 |
| 2½ | 73.03 | 10S | 3.05 | 5.35 |
| 2½ | 73.03 | 40S | 5.16 | 8.77 |
| 2½ | 73.03 | 80S | 7.01 | 11.59 |
| 3 | 88.9 | 10S | 3.05 | 6.56 |
| 3 | 88.9 | 40S | 5.49 | 11.47 |
| 3 | 88.9 | 80S | 7.62 | 15.51 |
| 3 | 88.9 | 160S | 11.132) | 21.67 |
| 3½ | 101.6 | 10S | 3.05 | 7.53 |
| 3½ | 101.6 | 40S | 5.74 | 13.78 |
| 3½ | 101.6 | 80S | 8.08 | 18.92 |
| 4 | 114.3 | 10S | 3.05 | 8.5 |
| 4 | 114.3 | 40S | 6.02 | 16.32 |
| 4 | 114.3 | 80S | 8.56 | 22.67 |
| 4 | 114.3 | 160S | 13.492) | 34.05 |
| 5 | 141.3 | 40S | 6.55 | 22.1 |
| 5 | 141.3 | 80S | 9.53 | 31.44 |
| 5 | 141.3 | 160S | 15.882) | 49.87 |
| 6 | 168.28 | 10S | 3.4 | 14.04 |
| 6 | 168.28 | 40S | 7.11 | 28.69 |
| 6 | 168.28 | 80S | 10.97 | 43.21 |
| 6 | 168.28 | 160S | 18.262) | 68.59 |
| 8 | 219.08 | 40S | 8.18 | 43.2 |
| 8 | 219.08 | 80S | 12.7 | 65.63 |
| 8 | 219.08 | 160S | 23.012) | 112.97 |
Zanglamaydigan po'latdan 2507 yetkazib beruvchiga moslashtirilgan xizmat
Huitong nufuzli sertifikati (ISO9001, Idoralar sertifikati, ASME sertifikati, EN sertifikati, SGS, BV uchinchi tomon sinovi) va 10+ yillik eksport tajribasiga ega bo'lgan po'lat quvur yetkazib beruvchi hisoblanadi. Biz mijozlarning o'ziga xos loyiha ehtiyojlariga muvofiq tayyorlangan super dupleks 2507 po'lat quvur echimlarini taqdim eta olamiz. Shu jumladan maxsus ishlov berish, hajmi, materiali, logotipi, sirtni qayta ishlash va qadoqlash talablari.
Bizning moslashtirish jarayoni:
Customers put forward requirements -> Technical team evaluates feasibility -> Provide customized solutions and quotations -> Confirm solutions -> Production and quality inspection ->Yetkazib berish.
Biz bilan bog'laning |market@htpipe.comqo'shimcha ma'lumot va bepul taklif uchun!
TSS
Savol: Siz namunalarni bepul taqdim etasizmi?
Savol: To'g'ri mahsulotlarni qidirish uchun qanday ma'lumotlarni taqdim etishim kerak?
Savol: Minimal buyurtma miqdori qancha?
Savol: kg uchun 2507 zanglamaydigan po'lat quvur narxi haqida?
Savol: Sizning yetkazib berish muddati qancha davom etadi?
Savol: Fabrikangizga tashrif buyurishim mumkinmi?
Savol: Mahsulot sifat nazorati bormi?
Savol: Eksport qilinadigan mamlakatlar
Issiq teglar: 2507 zanglamaydigan po'lat quvur, 2507 quvur, super dupleks 2507 quvur
Keyingi2
ASTM A790 UNS S32750 quvuriSizga ham yoqishi mumkin
So'rov yuborish