ASTM A789 dupleks zanglamaydigan po'lat quvur

ASTM A789 dupleks zanglamaydigan po'lat quvur


1. Standart: ASTM A789, ASME SA 789
2. Choksiz quvur hajmi: 1/2 "dan 8" gacha
3. Payvandlangan trubaning o'lchami: 6 "dan 24" gacha
4. Tashqi diametri: 6.0mm-630mm
5. Devor qalinligi: 1 mm dan 50 mm gacha
So'rov yuborish
Mahsulotni tanishtirish

ASTM A789 dupleks zanglamaydigan po'lat quvur,tarkibida taxminan 50% ferrit va 50% ostenit mavjud. ASTM A789 trubkasi neytral xlorid eritmasida va H2Sda 304L, 316L ostenitik zanglamaydigan po'latdan ko'ra yaxshiroq stress korroziyaga chidamliligiga ega. Bu quvur ayniqsa, -50 daraja F/+600 F daraja harorat oralig‘iga mos keladi. Biz 15+ eksport tajribasiga ega 2507 yetkazib beruvchimiz. Biz choksiz quvurlar va payvandlangan quvurlarni, shu jumladan kichik diametrlardan katta diametrgacha ta'minlay olamiz. Qo'shimcha ma'lumot va bepul takliflar uchun biz bilan bog'laning!

 

ASTM A789 dupleks po'lat quvur standarti:

  • ASTM A789: Umumiy xizmat ko'rsatish uchun choksiz va payvandlangan ferrit / ostenitik zanglamaydigan po'lat quvurlar uchun standart spetsifikatsiya

 

  • Baholar: S31803, S32205, S32750, S32760, S32550

 

  • ASME B36.19: Zanglamaydigan po'lat quvurlar uchun spetsifikatsiya
ASTM A789 Stainless Steel Tube Suppliers

ASTM A789 dupleks zanglamaydigan po'latdan yasalgan quvurlarning texnik xususiyatlari

Standart ASTM A789 / A789M, ASME SA789
Choksiz quvur va quvur o'lchami 1/2" dan 8" IN gacha
Payvandlangan quvur va quvur hajmi 6 "dan 24" gacha
Tashqi diametri 6.0-630mm
Jadvallar 5, 10, 20, 40, 40, 60, 80, 80, 100, 120, 140, 160, XXH.
Devor qalinligi 1 mm dan 50 mm gacha
Tugatish

Sayqallangan, AP (Tavlangan va Tuzlangan), BA (Yorqin va Tavlangan), MF

Shakl Dumaloq, kvadrat, to'rtburchaklar, gidravlik, tekis yoki "U" egilgan quvurlar va boshqalar.
Uzunlik Yagona tasodifiy, ikki marta tasodifiy va kesish uzunligi.
Oxiri To‘g‘ri uchi, qirrali uchi, pog‘onali

 

ASTM A789 standart o'lchovli bardoshlik

ASTM A789 Hajmi, tashqi
Diametri,
[mm]
Ruxsat etilgan o'zgarishlar, in
OD
Ruxsat etilgan o'zgarishlar, in
WT
Ruxsat etilgan o'zgarishlar, in
Uzunlik
Yupqa devor trubkasi
D<12.7 ±0,13 mm ±15% 3 mm ...
12.7-38.1 ±0,13 mm ±10% 3 mm WT<1.6mm
38.1-88.9 ±0,25 mm ±10% 5 mm WT<2.4mm
88.9-139.7 ±0,38 mm ±10% 5 mm WT<3.8mm
139.7-203.2 ±0,76 mm ±10% 5 mm WT<3.8mm

 

ASTM A789 dupleks zanglamaydigan po'lat quvur kimyoviy tarkibi

Baho C dan kichik yoki teng Mn dan kichik yoki teng P dan kichik yoki teng S dan kichik yoki teng Si dan kichik yoki teng Ni Cr Mo N Cu
S31803 0.03 2.00 0.03 0.02 1.00 4.5–6.5 21.0–23.0 2.5–3.5 0.08–0.20 -
S32205 0.03 2.00 0.03 0.02 1.00 4.5–6.5 22.0–23.0 3.0–3.5 0.14–0.20 -
S32750 0.03 1.20 0.035 0.02 0.80 6.0-8.0 24.0-26.0 3.0-5.0 0.24-0.32 0.5
S32760 0.05 1.00 0.03 0.01 1.00 6.0-8.0 24.0-26.0 3.0-4.0 0.20-0.30 0.50–1.00

 

ASTM A789 Materialning mexanik xususiyatlari

Mexanik xususiyatlar Uzilish, min, ksi[MPa] Hosildorlik, min, ksi[MPa] Uzayish, %(min) Qattiqlik, HB(maks)
S31803 90 [620] 65 [450] 25 290
S32205 95 [655] 65 [450] 25 290
S32750 116 [800] 80 [550] 15 300
S32760 109 [750] 80 [550] 25 300

 

ASTM A789 quvur issiqlik bilan ishlov berish

UNS belgisi Harorat darajasi F [ daraja] O'chirish
S31803 1870-2010℉(1020-1100 daraja) Havoda yoki suvda tez sovutish
S32205 1870-2010℉(1020-1100 daraja) Havoda yoki suvda tez sovutish
S32750 1880-2060℉(1025-1125 daraja) Havoda yoki suvda tez sovutish
S32760 2010-2085℉(1100-1140 daraja) Havoda yoki suvda tez sovutish

 

UNS S31803 va S32205 ning jismoniy xususiyatlari

Baho Zichlik
(kg/m3)
Elastik
Modul (GPa)
Issiqlikning o'rtacha koeffitsienti
Kengayish (mkm / m / daraja)
Termal
O'tkazuvchanlik (Vt/mK)
Maxsus
Issiqlik
0-100 daraja (J/kg.K)
Elektr
Qarshilik
(nΩ.m)
0-100 daraja 0-315 daraja 0-538 daraja 100 darajada 500 daraja haroratda
2205 782 190 13.7 14.2 - 19 - 418 850

 

ASTM A789 dupleks naychasining qo'llanilishi

  • Neft va gaz sanoati
  • Kimyo sanoati
  • Dengiz suvini tuzsizlantirish
  • Kanalizatsiya tozalash
  • Arxitektura va konstruktiv muhandislik

 

TSS

Savol: ASTM A789 dupleks zanglamaydigan po'latdan trubaning kg uchun narxi haqida?

Javob: Narxlar har bir kg uchun 6 dan 12 dollargacha o'zgaradi, o'lchamiga, devor qalinligiga, etkazib beruvchiga va hokazolarga qarab o'zgaradi.

Savol: Sizning yetkazib berish muddati qancha davom etadi?

Javob: Yetkazib berish muddati 5-21 kun ichida

Savol: Siz namuna bera olasizmi?

Javob: Namunalar bepul taqdim etiladi

Savol: MOQ nima?

Javob: Minimal buyurtma miqdori yo'q

Savol: Mahsulotlarni qanday qadoqlash kerak?

Javob: Ichki qatlam suv o'tkazmaydigan qog'oz tashqi qatlamiga ega va fumigatsiyali yog'och sxemasidan o'rnatiladi.

Savol: Siz allaqachon qancha mamlakatni eksport qildingiz?

Javob: Braziliya, Janubiy Afrika, Indoneziya, Hindiston, Singapur, Malayziya, Eron, Rossiya, BAA, Chili, Laos va boshqalar

 

 

Issiq teglar: astm a789 quvurlari, dupleks zanglamaydigan po'lat quvur, zanglamaydigan po'lat quvur