ASTM A815 S32750 (2507)tirsak super dupleks zanglamaydigan po'latdan yasalgan armatura. 90 daraja LR BW tirsagi ASME B16.9 standartiga mos keladi va quvur yo'nalishidagi 90 daraja o'zgarishlar uchun mo'ljallangan. ASTM A815 UNS S32750 xloriddan kelib chiqadigan stressli korroziya yorilishi, chuqurchalar va yoriqlar korroziyasiga mukammal qarshilikka ega. Chidamlilik va tortishish kuchi 304 yoki 316 kabi ostenitik zanglamaydigan po'latlardan yuqori. -50 darajadan 300 darajagacha bo'lgan haroratga bardosh beradi.
Biz etkazib beruvchilar nafaqat ta'minlaymizSuper Duplex 2507 quvurs, quvurlar, plastinka, choyshab, dumaloq bar, shuningdek, ishlab chiqarilgan quvur g'altaklari xizmati, albatta, quvur qismlari, gardishlar, mahkamlagichlar va boshqalarni o'z ichiga oladi Bepul namunalar taqdim etilishi mumkin. Bepul taklif uchun biz bilan bog'laning.
Spec A815 S32750 Super Duplex SS uzun radiusli tirsak
| Texnik xususiyatlari | ASME B16.9 Uzun radiusli tirsak |
|---|---|
| Hajmi | Choksiz ButtWeld Fittings: 1/2" - 10" Payvandlangan payvandlangan armatura: 1/2" - 48" |
| O'lchamlari | ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, BS4504, BS4504, BS1560, BS10 |
| Qalinligi | SCH10, SCH20, SCH30, STD SCH40, SCH60, XS, SCH 80, SCH 100, SCH 120, SCH 140, SCH 160, XXS NACE MR 01-75 bilan mavjud |
| Turlari | Choksiz / ERW / payvandlangan / ishlab chiqarilgan quvur qismlari |
| Turi | DN15-DN1200 |
| Ulanish | Payvandlash |
| Radius | R=1D, 2D, 3D, 5D, 6D, 8D, 10D yoki moslashtirilgan quvur qismlari |
| Hajmi diapazoni | ½" NB dan 24" gacha NB Sch 10s, 40s, 80s, 160s, XXS. (DN6~DN100) |
| Uzun radiusli ko'cha tirsagi | Burchak : 22,5 daraja, 30 daraja, 45 daraja, 90 daraja, 180 daraja, 1,0D, 1,5D, 2,0D, 2,5D, 3D, 4D, 5D, 6D, 7D-40D. Standart: ASME B16.9, ASME B16.28, ASME B16.25, MSS SP-75 DIN2605 JISB2311 JISB2312 JISB2313, BS, GB, ISO |
| Ishlab chiqarish | Push, Press, Forge, Cast va hokazo. |

ASME B16.5 uzun radius 90 daraja tirsak o'lchamlari
| NPS | O.D. D |
90 daraja Uzoq radius Markazdan-oxirigacha- A |
90 daraja 3D Markazdan-oxirigacha- A |
| 1/2 | 21.3 | 38 | - |
| 3/4 | 26.7 | 38 | 57 |
| 1 | 33.4 | 38 | 76 |
| 1¼ | 42.2 | 48 | 95 |
| 1½ | 48.3 | 57 | 114 |
| 2 | 60.3 | 76 | 152 |
| 2½ | 73 | 95 | 190 |
| 3 | 88.9 | 114 | 229 |
| 3½ | 101.6 | 133 | 267 |
| 4 | 114.3 | 152 | 305 |
| 5 | 141.3 | 190 | 381 |
| 6 | 168.3 | 229 | 457 |
| 8 | 219.1 | 305 | 610 |
| 10 | 273 | 381 | 762 |
| 12 | 323.8 | 457 | 914 |
| 14 | 355.6 | 533 | 1067 |
| 16 | 406.4 | 610 | 1219 |
| 18 | 457 | 686 | 1372 |
| 20 | 508 | 762 | 1524 |
| 22 | 559 | 838 | 1676 |
| 24 | 610 | 914 | 1829 |
| 26 | 660 | 991 | 1981 |
| 28 | 711 | 1067 | 2134 |
| 30 | 762 | 1143 | 2286 |
| 32 | 813 | 1219 | 2438 |
| 34 | 864 | 1295 | 2591 |
| 36 | 914 | 1372 | 2743 |
| 38 | 965 | 1448 | 2896 |
| 40 | 1016 | 1524 | 3048 |
| 42 | 1067 | 1600 | 3200 |
| 44 | 1118 | 1676 | 3353 |
| 46 | 1168 | 1753 | 3505 |
| 48 | 1219 | 1829 | 3658 |
Super Duplex 2507 quvur qismlari uchun asosiy ilovalar
Dengizdagi neft va gaz:Dengiz osti quvurlari tizimlari, yuqori texnologik quvurlar va qattiq dengiz muhitiga ta'sir qiladigan ko'taruvchi tizimlar.
Tuzsizlantirish zavodlari:Yuqori{0}}bosimli teskari osmos (RO) quvurlari va dengiz suvi olish tizimlari.
Kimyoviy va neft-kimyoni qayta ishlash:Organik kislotalar, xloridlar va nitrat kislota aralashmalari bilan ishlov berish uchun uskunalar.
Tutun gazini oltingugurtdan tozalash (FGD):Nam xlorid sharoitida ishlaydigan skrubber tizimlari.
HT PIPE dan sertifikatlangan ASTM A815 S32750 armatura buyurtma qiling
Zhengzhou Huitong Pipeline Equipment Co., Ltd. (HT PIPE)Super Duplex 2507 payvand choklari, soxta troyniklar, choksiz quvurlar va-prefabrik quvur g‘altaklarining to‘liq assortimentini ishlab chiqaradi va eksport qiladi.
Standartlarga muvofiqligi:ASME B16.9, ASME B16.28, MSS SP-43, NACE MR0175 / ISO 15156.
Sifatni tekshirish:100% PMI sinovidan o'tgan, radiografik test (RT), gidro-sinovdan o'tgan va EN 10204 3.1 / 3.2 bo'yicha sertifikatlangan.