ASTM A249 / A249M standarti
ASTM A249 standartiPayvandlangan ostenitik po'lat qozon, o'ta qizdirgich, issiqlik almashtirgich va kondensator quvurlari uchun spetsifikatsiya. ASTM A249 po'lati og'ir muhitda ishlatilishi mumkin va buzilishsiz yuqori haroratga yaxshi qarshilik ko'rsatadi. Uni nikel yoki titan kabi boshqa metallar bilan ham payvandlash mumkin. Bu kimyo, neft va oziq-ovqat sanoati kabi ko'plab ilovalar uchun ishlatiladigan yuqori quvvatli, past qotishma po'latdir.
ASTM A249 zanglamaydigan po'lat quvur ilovalari
ASTM A249 zanglamaydigan po'lat quvurlaruglevodorod va boshqa kimyo zavodlari, energiya ishlab chiqarish va kogeneratsiya zavodlari, suv va oqava suvlarni issiqlikni qayta tiklash tizimlari, noorganik sintez zavodlari, neftni qayta ishlash qurilmalari va boshqa turli sanoat ilovalari uchun mashhur tanlovdir.
Astm A249 quvurlari materiallari va darajasi
ASTM A249 Texnik xususiyatlari zanglamas po'latdan yasalgan oilalarda ishlatiladigan quvurlarning materiali ko'plab ilovalarda keng qo'llaniladigan Ostenitik zanglamaydigan po'latdan yasalgan navlar ekanligini ko'rsatadi.ASTM A249 TP304, TP304L, TP316 va TP316L sinflariUlarning barchasi turli xil ilovalar uchun ideal materiallardir, chunki ular boshqa po'latlarga ega bo'lmagan ko'plab afzalliklarga ega.
ASTM A249 TP304 zanglamaydigan po'lat quvurlarhar qanday bosim tizimining muhim qismidir va TIG payvandlash uchun talab qilinadi.ASTM A249 TP304L zanglamaydigan po'latdan payvandlangan quvurASTM standarti, 304L toifali zanglamaydigan po'lat va yorqin tavlanadigan qoplamaning texnik xususiyatlariga javob berish uchun ishlab chiqariladi. Quvur odatda isitish uskunalari, kondensatorlar va boshqa isitish tizimlari uchun ishlatiladi.
Agar siz og'ir sharoitlarda zanglamaydigan po'latdan yasalgan quvurlarning ishlash muddatini uzaytirmoqchi bo'lsangiz,ASTM A249 TP316/316L payvandlangan quvurlaryuqori korroziyaga chidamliligi va ichki va tashqi korroziyaga qarshilik ko'rsatish qobiliyati tufayli issiqlik almashinuvchilari, superheaterlar va qozonlar uchun ajoyib imkoniyatdir.
ASTM A249 Payvandlangan quvurlarning o'lchamlari, o'lchamlari va toleranslari
ASME SA 249 quvurihajmi va devor qalinligi: 1/8 dyuym (3,2 mm) ichki diametri 12 dyuym (3{7}}4,8 mm) tashqi diametri, 0.015 dyuym 0,32 dyuym (0,4) – 8,1 mm). Quvur o'lchamlari dyuym yoki millimetrda ifodalanadi, ba'zan esa spetsifikatsiyalar (BWG) ko'rsatiladi.
A249/A269 quvurlarining umumiy o'lchamlari
| O.D. | MM | DEVOR QALINLIGI | MM | UZUNLIKLAR | Baholar | Turi | XUSUSIYATLAR |
|---|---|---|---|---|---|---|---|
| 1/2" | 12.70 | 0.065" | 1.65 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 3/4" | 19.05 | 0.065" | 1.65 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 1" | 25.4 | 0.049" | 1.24 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 1" | 25.4 | 0.065" | 1.65 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 11/2" | 38.10 | 0.049" | 1.24 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 11/2" | 38.10 | 0.065" | 1.65 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 2" | 50.80 | 0.049" | 1.24 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 2" | 50.80 | 0.065" | 1.65 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 21/2" | 63.50 | 0.065" | 1.65 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 3" | 76.20 | 0.065" | 1.65 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 4" | 101.60 | 0.065" | 1.65 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 4" | 101.60 | 0.083" | 2.11 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 6" | 152.40 | 0.083" | 2.11 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 6" | 152.40 | 0.109" | 2.77 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 8" | 203.20 | 0.109" | 2.77 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 10" | 254.00 | 0.134" | 3.40 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
| 12" | 304.80 | 0.134" | 3.40 | 10′ – 20′ | 304/304L/316L | Payvandlangan | A249 / A269 / A270 |
Hajmi toleranslari
ASTM A249 payvandlangan quvuro'lchovli bardoshlik ASTM A1016 spetsifikatsiyasiga mos keladi, devor qalinligi bardoshliligi ASTM A269 trubkasi o'lchamiga nisbatan tolerantlik bilan taqqoslaganda, qalinligining +/-10% ni tashkil qiladi.
| OD | WTH | L | ||
|---|---|---|---|---|
| ASTM A249 | <25,40 mm | ±0.10mm | ±10.00% | OD<50,8mm +3,0mm -0mm OD 50,8 mm +5.0 -0 mm dan katta yoki unga teng |
| 25,4 mm ~ 38,1 mm dan katta yoki unga teng | ±0,15 mm | |||
| 38,1 mm ~ 50,8 mm dan katta yoki teng | ±0.20mm | |||
| 50,8 mm ~ 63,5 mm dan katta yoki unga teng | ±0,25 mm | |||
| 63,5 mm ~ 76,2 mm dan katta yoki unga teng | ±0.30mm | |||
| 76,2 mm ~ 101,6 mm dan katta yoki unga teng | ±0,38 mm | |||
| 101,6 mm ~ 190,5 mm dan katta yoki unga teng | +0.38mm -0.64mm | |||
| 190,5 mm ~ 228,6 mm dan katta yoki unga teng | +0.38mm -1.14mm | |||
| ASTM A269 | <38,1 mm | ±0,13 mm | OD<12,7mm ±15% OD 12,7 mm dan katta yoki unga teng ±10% |
OD<38,1 mm +3, 20 mm -0 mm OD 38,1 mm +4.80 -0 mm dan katta yoki unga teng |
| 38,1 mm ~ 88,9 mm dan katta yoki unga teng | ±0,25 mm | |||
| 88,9 mm ~ 139,7 mm dan katta yoki unga teng | ±0,38 mm | |||
| 139,7 mm ~ 203,7 mm dan katta yoki unga teng | ±0,76 mm | |||
| 203,7 mm ~ 304,8 mm dan katta yoki teng | ±1,01 mm | |||
| 304,8 mm ~ 355,6 mm dan katta yoki unga teng | ±1,26 mm | |||
Mexanik xususiyatlar
ASTM A249: tekislash, gardish va teskari egilish, valentlik sinovi va qattiqlik.
ASTM A269 va A249 o'rtasidagi farq nima?
ASTM A249 qozonxonalar yoki issiqlik almashtirgichlarda muhim muhitda foydalanish uchun keng qamrovli mexanik sinovlarni talab qiladi. ASTM A269 teskari tekislashni, shuningdek, gardish va qattiqlik sinovlarini talab qiladi. Bu kuchlanish sinovini talab qilmaydi. ASTM A270 faqat teskari tekislash testini talab qiladi.
ASTM A249 VS ASTM A269, farqi nimada?
| Parametr | ASTM A249 | ASTM 269 |
|---|---|---|
| Quvurlar ishlab chiqarish | Payvandlangan | Payvandlangan va choksiz |
| Ilova | Qozon O'ta qizdirgich Issiqlik almashtirgich Kondensator |
Umumiy xizmat |
| O'lchamlari | OD: Maks 304,8 mm Qalinligi: 0,4 – 8,1 mm |
ID: min. 3,4 mm Qalinligi: 0,51 mm |
| ASTM / ASME | ASTM A249 ASME SA249 |
ASTM A269 |
| Sinov | Flanj sinovi | Yonish sinovi |