ASTM A790 (ASME SA790) Choksiz va payvandlangan ferrit / ostenitik zanglamaydigan po'lat quvur uchun standart spetsifikatsiya. Quvur choksiz yoki avtomatik payvandlash usuli bilan amalga oshirilishi kerak, payvandlash jarayonida plomba metalli qo'shilmaydi. A790 talablariga javob berish uchun dupleks choksiz quvur va dupleks payvandlangan quvurlar kuchlanish sinovlari, qattiqlashuv sinovlari, tekislash sinovlari, gidrostatik sinovlar va buzilmaydigan elektr sinovlaridan o'tkazilishi kerak.
Ilovalar ASTM A790 dupleks zanglamaydigan po'lat quvurlari
Dengiz muhiti
Ifloslanishni nazorat qilish uskunalari
Neft va gazni qayta ishlash
Pulpa va qog'oz ishlab chiqarish
Neft va gaz qidiruvi va dengizdagi burmalar
Kimyoviy jarayon zavodi
Kimyoviy qayta ishlash, tashish va saqlash
ASTM A790 spetsifikatsiya darajalari mavjud:
UNS S31803 (Dupleks 2205, 1.4462, F51)
UNS S32205 (Dupleks 2205, 1.4462, F60)
UNS S32750 (2507, 1.4410, F53)
UNS S32760 (DIN1.4501, F55)
UNS S32550 (Ferralium 255, 1.4507, F61)
ASTM A790 quvurining sirt holati
Barcha ASTM A790 quvurlari ortiqcha tegirmon shkalasidan xoli bo'lishi va tekshirish uchun mos bo'lishi kerak. Oksidlanishning ozgina miqdori shkala sifatida qabul qilinmaydi. Har qanday maxsus tugatish talablari ishlab chiqaruvchi va xaridor o'rtasidagi kelishuvga bog'liq bo'lishi kerak.
ASTM A789 dupleks po'lat kimyoviy tarkibi
| Belgilash | C | Mn | P | S | Si | Ni | Cr | Mo | N | Cu | Boshqalar |
| S31803 | 0.03 | 2 | 0.03 | 0.02 | 1 | 4.5–6.5 | 21.0–23.0 | 2.5–3.5 | 0.08–0.20 | . . . | . . . |
| S32205 | 0.03 | 2 | 0.03 | 0.02 | 1 | 4.5–6.5 | 22.0–23.0 | 3.0–3.5 | 0.14–0.20 | . . . | . . . |
| S32750 | 0.03 | 1.2 | 0.035 | 0.02 | 0.8 | 6.0–8.0 | 24.0–26.0 | 3.0–5.0 | 0.24–0.32 | 0.5 | . . . |
| S32760 | 0.03 | 1 | 0.03 | 0.01 | 1 | 6.0–8.0 | 24.0–26.0 | 3.0–4.0 | 0.20–0.30 | 0.5 | W 0.50 |
| –1.00 | –1.00 | ||||||||||
| S32550 | 0.04 | 1.5 | 0.04 | 0.03 | 1 | 4.5–6.5 | 24.0–27.0 | 2.9–3.9 | 0.10–0.25 | 1.5 | . . . |
| –2.50 |
ASTM A790 standart issiqlik bilan ishlov berish
| UNS belgisi | Harorat | O'chirish |
| S31803 | 1870-2010 daraja F [1020-1100 daraja] | Havoda yoki suvda tez sovutish |
| S32205 | 1870-2010 daraja F [1020-1100 daraja] | Havoda yoki suvda tez sovutish |
| S32550 | 1900 daraja F [1040 daraja] min. | Havoda yoki suvda tez sovutish |
| S32750 | 1880-2060 daraja F [1025-1125 daraja] | Havoda yoki suvda tez sovutish |
| S32760 | 2010-2085 daraja F [1100-1140 daraja] | Havoda yoki suvda tez sovutish |