ASTM B443 Kirish
Nikel-xrom-molibden-kolumbiy qotishmasi va nikel-xrom-molibden-kremniy qotishma plastinka, varaq va tasma uchun standart spetsifikatsiya
ASTM B443 ASME SB 443 spetsifikatsiyasi prokatlangan nikel-xrom-molibden-kolumbiy qotishmasi (UNS No. N06625) va nikel-xrom-molibden-kremniy qotishmasi (UNS № N06219) plitalari, choyshablari va chiziqlarini o'z ichiga oladi. N06625 qotishmalari turli xil issiqlik bilan ishlov berish sharoitlarining ikki toifasida taqdim etilishi kerak: ASTM B443 1-sinf (tavlangan); va 2-darajali (eritma tavlangan).
ASTM B443 plastinka varaqlarining xususiyatlari
ASTM B443 standarti ikkita materialni o'z ichiga oladi: nikel-xrom-molibden-niobiy qotishmasi(Inconel 625 UNS N06625)va nikel-xrom-molibden-kremniy qotishmasi (UNS N06219). Ular orasida ASTM B443 Inconel 625 ko'proq ishlatiladigan qotishma hisoblanadi. Nikel va xrom elementlari ikkala qotishma ham oksidlanishga mukammal qarshilik ko'rsatadi. Molibden elementi materialning reduksiyaga chidamliligini ta'minlaydi. ASTM B443 UNS N06625 da niobiy qattiq eritmani mustahkamlashda muhim rol o'ynaydi, u qotishmaga ko'proq kuch beradi.
Asosiy material darajalari va issiqlik bilan ishlov berish
ASTM B443 UNS N06625 plastinka, qatlam va tasma ish muhitiga qarab ikkita alohida issiqlik bilan ishlov berish sharoitida taqdim etiladi:
- 1-sinf (tavlangan):Minimal 1600 daraja F (871 daraja) haroratda issiqlik bilan ishlov beriladi. 1-daraj odatda 1100 daraja F (593 daraja) gacha bo'lgan haroratlarda ishlaydigan ilovalar uchun tanlanadi, bu erda yuqori kuchlanish, charchoq kuchi va nam korroziyaga / chuqurlikka qarshilik talab qilinadi.
- 2-darajali (tavlangan eritma):2000 daraja F (1093 daraja) minimal haroratda keyingi barqarorlashtiruvchi ishlov berish bilan yoki unsiz issiqlik bilan ishlov beriladi. 2-daraja 1100 darajadan (593 daraja) yuqori bo'lgan xizmat ko'rsatish harorati uchun tavsiya etiladi, bu erda emirilish va kuchlanishning yorilishiga qarshilik talab qilinadi.
Xona haroratining kuchlanish xususiyatlari va issiqlik bilan ishlov berish
|
Mahsulot |
Kuchlanish Kuch, min, ksi (MPa) |
Hosildorlik kuchi (0,2% ofset), min, ksi (MPa) |
2 da cho'zilish dyuym yoki 50 mm (yoki 4D), min, % |
|---|---|---|---|
| 1-sinf UNS N06625 (Tavlangan) | |||
| Sovuq haddelenmiş varaq va tasma | 120 (827) | 60 (414) | 30 |
| Issiq haddelenmiş choyshab va 2,75 dyuym (70 mm) gacha bo'lgan issiq haddelenmiş plastinka, shu jumladan | 110 (758) | 55 (379) | 30 |
| 0,375 dyuym (9,5 mm) gacha bo'lgan sovuq haddelenmiş plastinka, shu jumladan | 110 (758) | 55 (379) | 30 |
| 2-sinf UNS N06625 (Tavlangan eritma) | |||
| Sovuq haddelenmiş varaq va tasma, issiq haddelenmiş varaq, sovuq haddelenmiş plastinka va issiq haddelenmiş plastinka |
100 (690) | 40 (276) | 30 |
| Belgilangan qalinligi, dyuym (mm) | O'rtacha og'irlikdagi ruxsat etilgan ortiqcha Nominal og'irliklar foizida ifodalangan |
|||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| 48 yoshgacha (1220) |
48 dan 60 gacha (1220 dan 1520), bundan mustasno |
60 dan 72 gacha (1520 dan 1830), bundan mustasno |
72 dan 84 gacha (1830 yildan 2130), bundan mustasno |
84 dan 96 gacha (2130 dan 2440), bundan mustasno |
96 dan 108 gacha (2440 dan 2740), bundan mustasno |
108 dan 120 gacha (2740 dan 3050), bundan mustasno |
120 dan 132 gacha (3050 gacha 3350), bundan mustasno |
132 dan 144 gacha (3350 gacha 3660), bundan mustasno |
144 dan 160 gacha (3660 gacha 4070), bundan mustasno |
|
| 3/16 dan 5/16 gacha (4,8 dan 7,9 gacha), bundan mustasno | 9.0 | 10.5 | 12.0 | 13.5 | 15.0 | 16.5 | 18.0 | ... | ... | ... |
| 5/16 dan 3/8 gacha (7,9 dan 9,5 gacha), bundan mustasno | 7.5 | 9.0 | 10.5 | 12.0 | 13.5 | 15.0 | 16.5 | 18.0 | ... | ... |
| 3/8 dan 7/16 gacha (9,5 dan 11,1 gacha), bundan mustasno | 7.0 | 7.5 | 9.0 | 10.5 | 12.0 | 13.5 | 15.0 | 16.5 | 18.0 | 19.5 |
| 7/16 dan 1/2 gacha (11,1 dan 12,7 gacha), bundan mustasno | 6.0 | 7.0 | 7.5 | 9.0 | 10.5 | 12.0 | 13.5 | 15.0 | 16.5 | 18.0 |
| 1/2 dan 5/8 gacha (12,7 dan 15,9 gacha), bundan mustasno | 5.0 | 6.0 | 7.0 | 7.5 | 9.0 | 10.5 | 12.0 | 13.5 | 15.0 | 16.5 |
| 5/8 dan 3/4 gacha (15,9 dan 19,1 gacha), bundan mustasno | 4.5 | 5.5 | 6.0 | 7.0 | 7.5 | 9.0 | 10.5 | 12.0 | 13.5 | 15.0 |
| 3/4 dan 1 gacha (19,1 dan 25,4 gacha), bundan mustasno | 4.0 | 4.5 | 5.5 | 6.0 | 7.0 | 7.5 | 9.0 | 10.5 | 12.0 | 13.5 |
| 1 dan 2 gacha (25,4 dan 50,8 gacha), shu jumladan | 4.0 | 4.0 | 4.5 | 5.5 | 6.0 | 7.0 | 7.5 | 9.0 | 10.5 | 12.0 |
Kimyoviy tarkibi (UNS N06625 va UNS N06219)
ASTM B443 materiallarining ajoyib korroziyaga chidamliligi va mustahkamligi ularning aniq qotishma kimyosidan kelib chiqadi. Niobiy (Kolumbiy) qarish issiqlik bilan ishlov berishni talab qilmasdan qattiq eritmani mustahkamlovchi sifatida ishlaydi.
| Element | UNS N06625 (Inconel 625) (%) | UNS N06219 (%) |
| Nikel (Ni) | 58.0 min | Balans |
| Xrom (Cr) | 20.0 – 23.0 | 18.0 – 22.0 |
| Molibden (Mo) | 8.0 – 10.0 | 7.0 – 9.0 |
| Niobiy + Tantal (Nb + Ta) | 3.15 – 4.15 | 0.20 – 0.70 |
| Temir (Fe) | 5.0 max | 2.0 – 6.0 |
| Silikon (Si) | 0.50 max | 1.50 – 2.50 |
| Uglerod (C) | 0.10 max | 0.05 max |
| Marganets (Mn) | 0.50 max | 0.50 max |
| Fosfor (P) / Oltingugurt (S) | 0,015 maksimal / 0,015 maksimal | 0,020 maksimal / 0,015 maksimal |
| Alyuminiy (Al) / Titan (Ti) | 0,40 maksimal / 0,40 maksimal | 0,50 maksimal / 0,50 maksimal |
Mavjud mahsulot shakllari va qo'shimcha qiymatli xizmatlar
Nikel qotishma mahsulotlarining global eksportchisi sifatida biz ASTM B443 / ASME SB 443 UNS N06625 materialini xalqaro standartlarga to'liq mos ravishda yetkazib beramiz:
Mavjud shakllar:Og'ir issiq haddelenmiş plitalar, sovuq haddelenmiş choyshablar, rulonlar, kesilgan chiziqlar va maxsus plazma / suv oqimi bilan kesish halqalari va disklari.
Yuzaki qoplamalar:Issiq haddelenmiş tavlangan va tuzlangan (№1 tugatish), sovuq haddelenmiş 2B, yorqin tavlangan (BA).
Sinov va tekshirish:UZ 10204 3.1 Tegirmon sinovi sertifikatlari (MTR), pozitiv material identifikatsiyasi (PMI), ultratovush tekshiruvi (ASTM A578 boʻyicha UT), mikro tuzilma tahlili va uchinchi tomon tekshiruvi (SGS, Bureau Veritas, TÜV).
Sertifikatlangan ASTM B443 UNS N06625 materiallarini qidiryapsizmi?
Bizda katta zaxiralar mavjudInconel 625 plitalari, choyshablar va chiziqlar1-sinf va 2-darajali issiqlik bilan ishlov berilgan sharoitlarda ham.
Tez global etkazib berish:Havo/dengiz yuklari dengizga yaroqli yog'och qutilarga qadoqlangan.
Maxsus ishlov berish:Suv oqimi bilan kesish, kesish, qirqish va maxsus quvur g'altaklarini oldindan ishlab chiqarish.
[Tezkor narxlar va MTR namunalari uchun texnik eksport guruhimizga murojaat qiling]