UNS N08925, UNS N08031, UNS N08932, UNS N08926, UNS N08354, UNS N08830 va UNS R20033 plastinka, varaq va tasma uchun spetsifikatsiya
ASTM B625 - bu ASTM International tomonidan nashr etilgan standart spetsifikatsiya bo'lib, u bir nechta nikel qotishmalaridan tayyorlangan plastinka, qatlam va chiziqlarni qamrab oladi. Ushbu qotishmalar korroziyaga chidamlilik, yuqori haroratga chidamlilik va boshqa o'ziga xos xususiyatlar juda muhim bo'lgan turli sanoat ilovalarida qo'llaniladi.
ASTM B625 nikel qotishma navlariKimyoviy tarkibi:
| Qotishma darajasi | (Ni) % | (Cr) % | (oy) % | (Cu) % | (Fe) % | (C) % | (Mn) % | (P) % | (Si) % | (S) % | Boshqa elementlar |
|---|---|---|---|---|---|---|---|---|---|---|---|
| UNS N08925 / qotishma 25-6MO | 42-46 | 19.5-21.5 | 6.0-7.0 | - | 22 min | 0 dan kichik yoki unga teng.03 | 2 dan kichik yoki teng.0 | 0 dan kichik yoki unga teng.03 | 0 dan kichik yoki unga teng.50 | 0 dan kichik yoki unga teng.01 | - |
| UNS N08031/ qotishma 31 | 30-32 | 24-26 | 6-7 | 1.4-2.6 | 42 min | 0 dan kichik yoki unga teng.015 | 2 dan kichik yoki teng.0 | 0 dan kichik yoki unga teng.03 | 0 dan kichik yoki unga teng.70 | 0 dan kichik yoki unga teng.01 | - |
| UNS N08932 | 32-38 | 19-21 | 2-3 | 3-4 | Bal. | 0 dan kichik yoki unga teng.06 | 2 dan kichik yoki teng.0 | 0 dan kichik yoki unga teng.03 | 1 dan kichik yoki unga teng.00 | 0 dan kichik yoki unga teng.03 | - |
| UNS N08926 / Qotishma 926 | 24-26 | 19-21 | 6-7 | 1.5-2.5 | Bal. | 0 dan kichik yoki unga teng.02 | 2 dan kichik yoki teng.0 | 0 dan kichik yoki unga teng.03 | 0 dan kichik yoki unga teng.50 | 0 dan kichik yoki unga teng.01 | - |
| UNS N08354 | 17.5-18.5 | 19.5-20.5 | 6-7 | 0.18-0.25 | Bal. | 0.020 dan kichik yoki unga teng | 1 dan kichik yoki unga teng.00 | 0 dan kichik yoki unga teng.03 | 0 dan kichik yoki unga teng.80 | 0 dan kichik yoki unga teng.01 | N 0.18-0.25 |
| UNS N08830 / Qotishma 330 | 34-37 | 19-21 | - | - | Bal. | 0 dan kichik yoki unga teng.05 | 2 dan kichik yoki teng.00 | 0 dan kichik yoki unga teng.03 | 1 dan kichik yoki unga teng.00 | 0 dan kichik yoki unga teng.03 | - |
| UNS R20033 | 58-63 | 20-24 | 8-10 | - | 3-5 | 0 dan kichik yoki unga teng.015 | 1 dan kichik yoki unga teng.00 | 0 dan kichik yoki unga teng.02 | 1 dan kichik yoki unga teng.00 | 0 dan kichik yoki unga teng.01 | - |
ASME SB 625Nikel qotishmalari navlariMexanik xususiyatlari:
| Qotishma darajasi | Hosildorlik kuchi (MPa) | Kuchlanish kuchi (MPa) | Cho'zilish (%) |
|---|---|---|---|
| UNS N08925 | 300 dan katta yoki unga teng | 650 dan katta yoki unga teng | 35 dan katta yoki teng |
| UNS N08031 | 280 dan katta yoki teng | 550 dan katta yoki teng | 35 dan katta yoki teng |
| UNS N08932 | 300 dan katta yoki unga teng | 650 dan katta yoki unga teng | 35 dan katta yoki teng |
| UNS N08926 | 300 dan katta yoki unga teng | 650 dan katta yoki unga teng | 35 dan katta yoki teng |
| UNS N08354 | 300 dan katta yoki unga teng | 690 dan katta yoki unga teng | 35 dan katta yoki teng |
| UNS N08830 | 205 dan katta yoki teng | 515 dan katta yoki unga teng | 40 dan katta yoki teng |
| UNS R20033 | 550 dan katta yoki teng | 690 dan katta yoki unga teng | 20 dan katta yoki teng |
ASTM B625 qotishmalari ilovalari:
- Kimyoviy ishlov berish: kislotalar va ishqorlar kabi korroziy kimyoviy moddalar bilan ishlov berish uchun uskunalar.
- Neft va gaz: og'ir muhitlarga, shu jumladan dengiz platformalariga ta'sir qiladigan komponentlar.
- Dengiz: dengiz suvi korroziyasiga chidamli materiallar.
- Energiya ishlab chiqarish: yuqori haroratlarda ishlaydigan qozon komponentlari va issiqlik almashinuvchilari.
- Pulpa va qog'oz: qog'ozni qayta ishlashda korroziy muhitga qarshilik.
- Tuzsizlantirish: Dengiz suvini tuzsizlantirish zavodlarida ishlatiladigan materiallar.