ASTM A213 SS 310 trubkasi

ASTM A213 SS 310 trubkasi



1. Standart: ASTM A213, ASME SA213
2. OD hajmi: 1/8" OD (3,18 mm) - 5" OD (127 mm)
3. Devor qalinligi: 0.40 mm - 12.70 mm
4. Ekvivalenti: UNS S31000, WNR.1.4841, AISI 310
So'rov yuborish
Mahsulotni tanishtirish

ASTM A213 SS 310 trubkasiyuqori haroratli qotishma bo'lib, u 1100 darajagacha bo'lgan haroratga bardosh bera oladi va yuqori haroratli muhitda oksidlanish va korroziyaga mukammal qarshilik ko'rsatadi. SS S31000 trubkasi yuqori foizli xrom (odatda taxminan 25-28%) va nikel (taxminan 19-22%) o'z ichiga oladi, bu unga mukammal issiqlikka chidamlilik va sulfidlanish va karburizatsiyaga mukammal qarshilik ko'rsatadi. SS 310 choksiz trubkasida payvand choki yo'q va payvandlangan quvurlarga qaraganda kuchliroq bosim qarshiligiga ega. Biz birQotishma 31015+ eksport tajribasiga ega yetkazib beruvchi, qoʻshimcha maʼlumot va narxlarni bepul olish uchun biz bilan bogʻlaning!

 

1.4841 AISI 310 zanglamas po'latdan yasalgan quvur ilovalari:

 

  • Pech komponentlari
  • Issiqlik almashinuvchilari
  • Pechlar va radiatsiya quvurlari
  • Neft-kimyo
  • Kimyo sanoati
  • Energiya ishlab chiqarish sanoati
310 stainless steel tube suppliers

 

SS 310 zanglamas po'latdan yasalgan quvurlarning texnik xususiyatlari

Spetsifikatsiya

ASTM A213 / ASME SA213

Hajmi

ASTM va ASME

Turi

Choksiz ferrit va ostenitik qozon, o'ta qizdirgich va issiqlik almashtirgich quvurlari

Tashqi diametri o'lchami

1/8 "OD, NB dan 5" OD gacha, NB o'lchamlari

Qalinligi

0,4 mm dan 12,7 mm gacha

Uzunlik

6 metrgacha, maxsus kesilgan uzunliklar

Tugaydi

№1 tuzlangan qoplama, №4 tugatish, BA tugatish, elektropolislangan choksiz quvurlar

Yetkazib berish shartlari

O'ralgan, shakllangan, stressdan xalos bo'lgan, tavlangan, qotib qolgan, qattiqlashtirilgan, sovuq chizish

Qoplama

Elektropolish, mexanik jilo, atlas qoplamasi, passivlangan

Boshqa testlar

Ko'ndalang kuchlanish testi, tekislash testi, don o'lchami testi, etching testi, radiografik tekshiruv, stabillashtiruvchi issiqlik bilan ishlov berish va boshqalar.

Qo'shilgan qiymat xizmatlari

Chizish / Kengaytirish / Ishlov berish / Qumni portlatish / Otishma / Issiqlik bilan ishlov berish

Qadoqlash

Bo'shashmasdan / to'plam / yog'och sxemasidan / yog'och quti / plastmassa mato o'ramlari / plastik qopqoq / qirrali himoya

Hozir bog'laning

ASTM A213 SS 310 issiqlik almashtirgichlar, kondensatorlar va qozon uchun quvurlar o'lchamlari

Tashqi diametri BWG
22 20 18 16 14 12 10
Devor qalinligi mm
0.71 0.89 1.24 1.65 2.11 2.77 3.4
mm dyuym Og'irligi kg/m
6.35 1/4 0.109 0.133 0.174 0.212 - - -
9.53 3/8 0.157 0.193 0.257 0.356 0.429 - -
12.7 1/2 0.214 0.263 0.356 0.457 0.612 0.754 -
15.88 5/8 0.271 0.334 0.455 0.588 0.796 0.995 -
19.05 3/4 0.327 0.405 0.553 0.729 0.895 1.236 -
25.4 1 0.44 0.546 0.75 0.981 1.234 1.574 2.05
31.75 1 1/4 0.554 0.688 0.947 1.244 1.574 2.014 2.641
38.1 1 1/2 0.667 0.832 1.144 1.514 1.904 2.454 3.233
44.5 1 3/4 - - 1.342 1.774 2.244 2.894 3.5
50.8 2 - - 1.549 2.034 2.574 3.334 4.03
63.5 2 1/2 - - 1.949 2.554 3.244 4.214 5.13
76.2 3 - - 2.345 3.084 3.914 5.094 6.19
88.9 3 1/2 - - 2.729 3.609 4.584 5.974 7.27
101.6 4 - - - 4.134 5.254 6.854 8.35
114.3 4 1/2 - - - 4.654 5.924 7.734 9.43

 

ASTM A213 TP310 choksiz quvurlarga chidamlilik

Spetsifikatsiya Ruxsat etilgan tashqi diametrning o'zgarishi (mm) Ruxsat etilgan devor qalinligi o'zgarishi (%) Aniq uzunlik bardoshlik (mm)
Nominal diametri tugadi ostida tugadi ostida tugadi ostida
ASTM A213 25.4 dan past 0.1016 0.1016 20 0 3.175 0
25.4-38.1, shu jumladan 0.1524 0.1524 22 0 3.175 0
38.1-50.8 bundan mustasno 0.2032 0.2032 22 0 3.176 0
50.8-63.5 bundan mustasno 0.254 0.254 22 0 4.46 0
63.5-76.2 bundan mustasno 0.3108 0.3108 22 0 4.76 0
76.2-101.6, shu jumladan 0.381 0.381 22 0 4.76 0

 

TSS

Savol: ASTM A213 SS 310 quvurlari narxlari haqida?

Javob: Narxlar har bir kilogramm uchun 5 dan 10 dollargacha, o'lchamiga, devor qalinligiga, etkazib beruvchiga va hokazolarga qarab o'zgaradi.

Savol: Sizning yetkazib berish muddati qancha davom etadi?

Javob: Yetkazib berish muddati 5-21 kun ichida

Savol: Namuna xizmati bormi?

Javob: Namunalar bepul taqdim etiladi

Savol: Minimal buyurtma miqdori qancha?

Javob: Minimal buyurtma miqdori yo'q

Savol: Mahsulotlarni qanday qadoqlash kerak?

Javob: Ichki qatlam suv o'tkazmaydigan qog'oz tashqi qatlamiga ega va fumigatsiyali yog'och sxemasidan o'rnatiladi.

Savol: Eksport qilinadigan mamlakatlar

Javob: Braziliya, Janubiy Afrika, Indoneziya, Hindiston, Singapur, Malayziya, Eron, Rossiya, BAA, Chili, Laos va boshqalar

 

 

 

Issiq teglar: 310 zanglamaydigan po'lat quvur, astm 310 zanglamaydigan po'lat, 310 zanglamaydigan quvur, 310 ss quvur

So'rov yuborish

whatsapp

Telefon

Elektron pochta