ASTM A269 317 zanglamaydigan po‘lat quvur

ASTM A269 317 zanglamaydigan po‘lat quvur



1. Standart: ASTM A269 / ASME SA269
2. OD: 3.00 mm - 219,10 mm
3. Qalinligi: 0.40 mm - 12.70 mm
4. Ekvivalenti: UNS S31700, WNR.1.4449, AISI 317
So'rov yuborish
Mahsulotni tanishtirish

ASTM A269 317 zanglamaydigan po‘lat quvurmolibden o'z ichiga olgan ostenitik zanglamaydigan po'latdir, 304 va 316 kabi standart zanglamaydigan po'latdan ko'ra yuqori darajadagi xrom, nikel va molibden.SS 317ayniqsa, sulfat kislota, xlorid kislotasi va nordon gazlarni o'z ichiga olgan xlorid o'z ichiga olgan muhitda mukammal korroziyaga chidamliligiga ega.1.4449 AISI 317 quvurlarimukammal oksidlanish qarshiligiga ega.317 SS trubkasikimyoviy, neft va gaz ilovalari uchun javob beradi. Biz zanglamas po'latdan yasalgan quvurlar yetkazib beruvchimiz, 15+ eksport tajribasiga egamiz, qo'shimcha ma'lumot va bepul narxlar uchun biz bilan bog'laning!

 

ASTM A269 317 zanglamaydigan po‘lat quvurlar standarti:
  • ASTM A269: Umumiy xizmat ko'rsatish uchun choksiz va payvandlangan ostenitik zanglamaydigan po'lat quvurlar uchun standart spetsifikatsiya

 

  • ASME B36.19: Zanglamaydigan po'lat quvurlar uchun spetsifikatsiya

 

  • Boshqa navlar: 310, 310S, 317, 317L, 321, 321H, 347, 347H, 904L, 254SMO, 253MA, S32550, S32205, S31803, 2507, S310c.
ASTM A269 317 stainless steel tubing suppliers

TP317 zanglamaydigan po'lat quvur spetsifikatsiyasi

Spetsifikatsiya

ASTM A-269 va uning ekvivalenti ASME, DIN va EN standarti.

Turi

Choksiz / payvandlangan / ERW / EFW / sovuq chizish / issiq tugatish / sovuq tugatish

Tashqi diametri o'lchami

  • Choksiz - 6 MM OD dan 114,3 MM OD gacha
  • - 10 MM dan 114,3 mm OD gacha payvandlangan

Devor qalinligi

0.8 MM TO 4 MM DEVOR QALINLIGI

Uzunlik

01 metrdan 12,5 metrgacha, bitta tasodifiy uzunlik, ikki marta tasodifiy uzunlik va moslashtirilgan o'lcham.

Tugaydi

Oddiy uchlari / qiyshiq uchlari

Hozir bog'laning

ASTM A269 SS 317 choksiz naychaning kimyoviy tarkibi

Baho C Ni Si N S Mn P Cr Mo
SS 317 min. 11.0 18.0 3.00
maks. 0.008 14.0 1.00 0.03 2.00 0.040 20.0 4.00

 

ASTM A269 UNS S31700 zanglamaydigan po'latdan sifat kafolati

  • Vizual tekshirish
  • O'lchovli tekshiruv
  • Chidamlilik sinovi
  • Qattiqlik sinovi
  • Gidrostatik sinov
  • Buzilmaydigan elektr sinovi

 

 

ASTM A269 TP317 SS quvurlari o'lchamlari

Tashqi diametri, dyuym

ID

BW
Ga.

Og'irligi
Lbs/Ft.

Devor
Dek. In.

1/8

00.069

22

00.0290

00.028

00.055

20

00.0336

00.035

3/16

00.131

22

00.0478

00.028

1/4

00.210

25

00.0491

00.020

00.194

22

00.0664

00.028

00.187

21

00.0745

00.032

00.180

20

00.0804

00.035

00.152

18

00.1052

00.049

00.120

16

00.1284

00.065

5/16

00.242

20

00.1039

00.035

00.214

18

00.1382

00.049

00.182

16

00.1722

00.065

3/8

00.319

22

00.1038

00.028

00.305

20

00.1271

00.035

00.277

18

00.1706

00.049

00.245

16

00.2152

00.065

7/16

00.340

18

00.2036

00.049

1/2

00.460

25

00.1025

00.020

00.430

20

00.1738

00.035

00.402

18

00.2360

00.049

00.370

16

00.3020

00.065

5/8

00.555

20

00.2205

00.035

00.527

18

00.3014

00.049

00.495

16

00.3888

00.065

3/4

00.680

20

00.2673

00.035

00.652

18

00.3668

00.049

00.620

16

00.4755

00.065

00.584

14

00.5913

00.083

7/8

00.777

18

00.4323

00.049

00.745

16

00.5623

00.065

00.635

11

00.9676

00.120

1

00.930

20

00.3607

00.035

00.902

18

00.4977

00.049

00.870

16

00.6491

00.065

00.834

14

00.8129

00.083

00.760

11

1.1278

00.120

1-1/4

1.010

11

1.4480

00.120

 

TSS

Savol: ASTM A269 317 zanglamaydigan po‘lat quvurlari narxlari haqidami?

Javob: Narxlar har bir kilogramm uchun 5 dan 10 dollargacha, o'lchamiga, devor qalinligiga, etkazib beruvchiga va hokazolarga qarab o'zgaradi.

Savol: Sizning yetkazib berish muddati qancha davom etadi?

Javob: Yetkazib berish muddati 5-21 kun ichida

Savol: Namuna xizmati bormi?

Javob: Namunalar bepul taqdim etiladi

Savol: Minimal buyurtma miqdori qancha?

Javob: Minimal buyurtma miqdori yo'q

Savol: Mahsulotlarni qanday qadoqlash kerak?

Javob: Ichki qatlam suv o'tkazmaydigan qog'oz tashqi qatlamiga ega va fumigatsiyali yog'och sxemasidan o'rnatiladi.

Savol: Eksport qilinadigan mamlakatlar

Javob: Braziliya, Janubiy Afrika, Indoneziya, Hindiston, Singapur, Malayziya, Eron, Rossiya, BAA, Chili, Laos va boshqalar

 

 

Issiq teglar: 317 zanglamaydigan po'lat quvurlar, zanglamaydigan po'latdan 317, a269 zanglamaydigan po'lat quvurlar

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov