ASTM A269 TP304 zanglamaydigan po'lat quvur

ASTM A269 TP304 zanglamaydigan po'lat quvur



1. Standart: ASTM A269, ASME SA269
2. OD: 6.0mm -500.0mm
3. Devor qalinligi: 0.6mm -12.7mm
4. Uzunlik: bitta tasodifiy uzunlik, ikki marta tasodifiy uzunlik va moslashtirilgan
So'rov yuborish
Mahsulotni tanishtirish

ASTM A269 TP304 zanglamaydigan po'lat quvurjuda yuqori korroziyaga chidamliligi, yaxshi ishlov berish va payvandlash qobiliyatiga ega. Amaldagi harorat oralig'iASTM A269 GR TP304 choksiz quvur-325 daraja F va 1500 daraja F (-198 darajadan 816 darajagacha) orasida va u yuqori harorat va ekstremal sharoitlarga bardosh bera oladi. Shuning uchun,qotishma 304suv, oksidlovchi moddalar, kislotalar va ishqorlar kabi yuqori haroratli korroziy muhitda foydalanish mumkin. Kompaniyamiz 15+ eksport tajribasiga ega zanglamaydigan poʻlat quvurlar yetkazib beruvchi hisoblanadi. Qo'shimcha ma'lumot va narxlarni bepul olish uchun biz bilan bog'laning!

 

ASTM A269 TP304 zanglamaydigan po'lat quvurlari standarti:

  • ASTM A269: Umumiy xizmat ko'rsatish uchun choksiz va payvandlangan ostenitik zanglamaydigan po'lat quvurlar uchun standart spetsifikatsiya

 

  • ASTM A249: Payvandlangan ostenitik po'lat qozon, o'ta qizdirgich, issiqlik almashtirgich va kondensator quvurlari uchun standart spetsifikatsiya

 

  • Sinflar: 316, 316L, 316Ti, 316L Mod, 17-4ph, 310, 310S, 317, 317L, 321, 321H, 347, 347H, 904L, 254SMO, 25325, S380, S380 7, S31050, S30815 va boshqalar.
ASTM A269 TP304 stainless steel tubing suppliers

ASTM A269 TP304 quvurining spetsifikatsiyasi

Spetsifikatsiya ASTM A269, ASME SA269
Shakllar Shlangi, dumaloq, U shakli, o'ralgan
Ishlab chiqarish turi Tayyorlangan / Choksiz / ERW / EFW / Payvandlangan
Yuzaki tugatish BA, 2B, №8, №1, №4, №3, 8K, 2D, 1D, HL, 400G
Qalinligi diapazoni SCH XXS, SCH 10, SCH XXH, SCH 5, SCH 40, SCH XS, SCH 80S, SCH 160, SCH 80
Texnika Sovuq chizilgan, Sovuq haddelenmiş, Ekstruziya, Issiq haddelenmiş quvur
Standart ASTM, GB, DIN, JIS, AISI, EN, SUS
OXIRI Qiyshiq uchi, oyoqli, tekis uchi
Qayta ishlash xizmati Kesish, ochish, bukish, payvandlash, teshish, qoliplash
Yetkazib berish sharti Sayqallangan, sovuq tortilgan, tavlangan va tuzlangan (AP), MF, yorqin tavlangan (BA)
Qadoqlash Yengli, yog'och qutili, uchlari yopilgan

Hozir bog'laning

ASTM A269 304 zanglamaydigan po‘latdan yasalgan quvurlar uchun ilova

  • Neft-kimyo
  • Oziq-ovqat
  • Farmatsevtika
  • Aerokosmik
  • Atrof-muhitni muhofaza qilish sohasi
  • Yarimo'tkazgich
  • Nozik mashinalar

 

SS 304 quvurlarni qayta ishlash samaradorligi

1.4301 304 zanglamaydigan po'lat quvur turli xil murakkab shakllarning ehtiyojlarini qondirish uchun ekstruziya, sovuq chizish, sovuq haddeleme va sovuq bükme orqali qayta ishlanishi mumkin.

 

AISI 304 zanglamaydigan quvur yetkazib beruvchi

HT PIPE professional zanglamaydigan po'latdan ASTM A269 UNS S30400 yetkazib beruvchi va ishlab chiqaruvchisi. Shuningdek, biz 304 zanglamaydigan po'latdan yasalgan armatura, gardishlar, mahkamlagichlar, quvurlar, quvurlar, plitalar, choyshablar, chiziqlar, novdalar va boshqalarni etkazib beramiz.

 

ASME SA269 TP304 quvurining bosim darajasi

Devor qalinligi dyuymlarda Dyuymdagi tashqi diametri Minimal tortishish kuchi (PSI) Minimal rentabellik kuchi (PSI) Ish bosimi Nazariy portlash bosimi Nazariy rentabellik nuqtasi Yiqilish bosimi
0.020 0.250 75,000 30,000 3,571 14,286 5,714 4,416
0.028 0.250 75,000 30,000 5,412 21,649 8,660 5,967
0.035 0.250 75,000 30,000 7,292 29,167 11,667 7,224
0.049 0.250 75,000 30,000 12,089 48,355 19,342 9,455
0.065 0.250 75,000 30,000 20,313 81,250 32,500 11,544
0.020 0.375 75,000 30,000 2,239 8,955 3,582 3,029
0.028 0.375 75,000 30,000 3,292 13,166 5,266 4,145
0.035 0.375 75,000 30,000 4,303 17,213 6,885 5,077
0.049 0.375 75,000 30,000 6,634 26,534 10,614 6,816
0.065 0.375 75,000 30,000 9,949 39,796 15,918 8,597
0.020 0.500 75,000 30,000 1,630 6,522 2,609 2,304
0.028 0.500 75,000 30,000 2,365 9,459 3,784 3,172
0.035 0.500 75,000 30,000 3,052 12,209 4,884 3,906
0.049 0.500 75,000 30,000 4,571 18,284 7,313 5,304
0.065 0.500 75,000 30,000 6,588 26,351 10,541 6,786
0.083 0.500 75,000 30,000 9,319 37,275 14,910 8,307
0.020 0.625 75,000 30,000 1,282 5,128 2,051 1,859
0.028 0.625 75,000 30,000 1,845 7,381 2,953 2,568
0.035 0.625 75,000 30,000 2,365 9,459 3,784 3,172
0.049 0.625 75,000 30,000 3,487 13,947 5,579 4,335
0.065 0.625 75,000 30,000 4,924 19,697 7,879 5,591
0.083 0.625 75,000 30,000 6,781 27,124 10,850 6,910
0.095 0.625 75,000 30,000 8,190 32,759 13,103 7,734
0.109 0.625 75,000 30,000 10,043 40,172 16,069 8,639
0.028 0.750 75,000 30,000 1,513 6,052 2,421 2,156
0.035 0.750 75,000 30,000 1,930 7,721 3,088 2,669
0.049 0.750 75,000 30,000 2,818 11,273 4,509 3,664
0.065 0.750 75,000 30,000 3,931 15,726 6,290 4,749
0.083 0.750 75,000 30,000 5,330 21,318 8,527 5,905
0.095 0.750 75,000 30,000 6,362 25,446 10,179 6,637
0.109 0.750 75,000 30,000 7,683 30,733 12,293 7,453
0.120 0.750 75,000 30,000 8,824 35,294 14,118 8,064
0.020 0.875 75,000 30,000 898 3,593 1,437 1,340
0.028 0.875 75,000 30,000 1,282 5,128 2,051 1,859
0.035 0.875 75,000 30,000 1,630 6,522 2,609 2,304
0.049 0.875 75,000 30,000 2,365 9,459 3,784 3,172
0.065 0.875 75,000 30,000 3,272 13,087 5,235 4,126
0.083 0.875 75,000 30,000 4,390 17,560 7,024 5,152
0.095 0.875 75,000 30,000 5,201 20,803 8,321 5,807
0.109 0.875 75,000 30,000 6,221 24,886 9,954 6,543
0.120 0.875 75,000 30,000 7,087 28,346 11,339 7,100
0.028 1.000 75,000 30,000 1,112 4,449 1,780 1,633
0.035 1.000 75,000 30,000 1,411 5,645 2,258 2,027
0.049 1.000 75,000 30,000 2,037 8,149 3,259 2,796
0.065 1.000 75,000 30,000 2,802 11,207 4,483 3,647
0.083 1.000 75,000 30,000 3,732 14,928 5,971 4,567
0.095 1.000 75,000 30,000 4,398 17,593 7,037 5,159
0.109 1.000 75,000 30,000 5,227 20,908 8,363 5,827
0.120 1.000 75,000 30,000 5,921 23,684 9,474 6,336
0.134 1.000 75,000 30,000 6,865 27,459 10,984 6,963
0.035 1.250 75,000 30,000 1,112 4,449 1,780 1,633
0.049 1.250 75,000 30,000 1,595 6,380 2,552 2,260
0.065 1.250 75,000 30,000 2,176 8,705 3,482 2,958
0.083 1.250 75,000 30,000 2,871 11,485 4,594 3,719
0.095 1.250 75,000 30,000 3,361 13,443 5,377 4,213
0.109 1.250 75,000 30,000 3,961 15,843 6,337 4,776
0.120 1.250 75,000 30,000 4,455 17,822 7,129 5,207
0.134 1.250 75,000 30,000 5,117 20,468 8,187 5,742
0.035 1.500 75,000 30,000 918 3,671 1,469 1,367
0.049 1.500 75,000 30,000 1,311 5,243 2,097 1,896
0.065 1.500 75,000 30,000 1,779 7,117 2,847 2,487
0.083 1.500 75,000 30,000 2,333 9,333 3,733 3,136
0.095 1.500 75,000 30,000 2,719 10,878 4,351 3,559
0.109 1.500 75,000 30,000 3,188 12,754 5,101 4,043
0.120 1.500 75,000 30,000 3,571 14,286 5,714 4,416
0.134 1.500 75,000 30,000 4,079 16,315 6,526 4,881
0.148 1.500 75,000 30,000 4,610 18,439 7,375 5,336
0.035 1.750 75,000 30,000 781 3,125 1,250 1,176
0.049 1.750 75,000 30,000 966 3,864 1,546 1,434
0.065 1.750 75,000 30,000 1,505 6,019 2,407 2,146
0.083 1.750 75,000 30,000 1,965 7,860 3,144 2,711
0.095 1.750 75,000 30,000 2,284 9,135 3,654 3,080
0.109 1.750 75,000 30,000 2,668 10,672 4,270 3,504
0.120 1.750 75,000 30,000 2,980 11,921 4,768 3,832
0.134 1.750 75,000 30,000 3,391 13,563 5,425 4,242
0.148 1.750 75,000 30,000 3,817 15,268 6,107 4,645
0.165 1.750 75,000 30,000 4,357 17,430 6,972 5,124
0.035 2.000 75,000 30,000 680 2,720 1,088 1,032
0.049 2.000 75,000 30,000 966 3,864 1,546 1,434
0.065 2.000 75,000 30,000 1,303 5,214 2,086 1,887
0.083 2.000 75,000 30,000 1,697 6,788 2,715 2,387
0.095 2.000 75,000 30,000 1,968 7,873 3,149 2,715
0.109 2.000 75,000 30,000 2,294 9,175 3,670 3,092
0.120 2.000 75,000 30,000 2,557 10,227 4,091 3,384
0.134 2.000 75,000 30,000 2,901 11,605 4,642 3,751
0.148 2.000 75,000 30,000 3,257 13,028 5,211 4,111
0.165 2.000 75,000 30,000 3,705 14,820 5,928 4,542

 

TSS

Savol: ASTM A269 TP304 zanglamaydigan po'lat quvurlar narxi haqida?

Javob: Narxlar har bir kilogramm uchun 5 dan 7 dollargacha, o'lchamiga, devor qalinligiga, etkazib beruvchiga va hokazolarga qarab o'zgaradi.

Savol: Sizning yetkazib berish muddati qancha davom etadi?

Javob: Yetkazib berish muddati 5-21 kun ichida

Savol: Namuna xizmati bormi?

Javob: Namunalar bepul taqdim etiladi

Savol: Minimal buyurtma miqdori qancha?

Javob: Minimal buyurtma miqdori yo'q

Savol: Mahsulotlarni qanday qadoqlash kerak?

Javob: Ichki qatlam suv o'tkazmaydigan qog'oz tashqi qatlamiga ega va fumigatsiyali yog'och sxemasidan o'rnatiladi.

Savol: Eksport qilinadigan mamlakatlar

Javob: Braziliya, Janubiy Afrika, Indoneziya, Hindiston, Singapur, Malayziya, Eron, Rossiya, BAA, Chili, Laos va boshqalar

 

 

Issiq teglar: 304 zanglamaydigan po'lat quvur, zanglamaydigan 304 quvur, astm a269 tp304, ss304 quvur

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov