ASTM A312 904L zanglamaydigan po'lat quvur

ASTM A312 904L zanglamaydigan po'lat quvur



1. Standart: ASTM A312 / ASME SA312
2. Hajmi: 1/8" NB - 24" NB
3. OD: 6.00 mm OD dan 914,4 mm gacha
4. Qalinligi: 0.3mm - 50 mm
So'rov yuborish
Mahsulotni tanishtirish

ASTM A312 904L zanglamaydigan po'lat quvursulfat kislota kabi kuchli qaytaruvchi kislotalarga chidamliligini oshirish uchun mis qo'shilgan past uglerodli zanglamaydigan po'latdir.SS 904L quvuriturli spetsifikatsiyalar va o'lchamlarda mavjud va choksiz yoki payvandlangan bo'lishi mumkin. 904L zanglamaydigan po'latdan yasalgan choksiz quvur qattiq novda teshilishi orqali ishlab chiqariladi va bosimga payvandlangan quvurga qaraganda yaxshiroq bardosh bera oladi. Lekin choksiz quvurlar payvandlangan quvurlarga qaraganda qimmatroq va katta diametrli quvur tizimlari uchun ko'proq mos keladi. 904L toifasi magnit bo'lmagan. Biz 15+ eksport tajribasiga ega AISI 904l yetkazib beruvchimiz, qoʻshimcha maʼlumot va bepul narxlar uchun biz bilan bogʻlaning!

 

ASTM A312 TP904L zanglamaydigan po'lat quvur standarti:

  • ASTM A312: Choksiz, payvandlangan va og'ir sovuq ishlov berilgan ostenitik zanglamaydigan po'lat quvurlar uchun standart spetsifikatsiya

 

  • Sinflar: TP304, TP304L, TP310S, TP316, TP316L , 316Ti, TP317, TP317L, TP321, TP347, TP347H, S31254, N08367, N08926, N08924,

 

  • ANSI B36.19: Zanglamaydigan po'lat quvurlar uchun spetsifikatsiya
904L Stainless Steel Pipe

ASTM A312 904L zanglamaydigan po‘lat quvurlarning texnik xususiyatlari

Spetsifikatsiya ASTM A312 / ASME SA312
Standart ASTM, ASME va API
Hajmi 1/8" NB - 24" NB
Turlari Choksiz / payvandlangan, issiq haddelenmiş / sovuq chizilgan
Uzunlik Yagona tasodifiy, ikki marta tasodifiy va talab qilinadigan uzunlik
Tashqi diametri 6.00 mm OD 914,4 mm gacha, oʻlchami 24” NB gacha
Qalinligi 0.3mm – 50 mm
Jadval SCH 5, SCH10, SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Shakl Dumaloq quvurlar, kvadrat quvurlar, to'rtburchaklar quvurlar, issiq tugatish quvurlari, sovuq chizilgan quvurlar,
Oxiri To‘g‘ri uchi, qirrali uchi, pog‘onali

Hozir bog'laning

SS 904L MEXANIK XUSUSIYATLARI:

Zichlik 7,95 g/sm3
Erish nuqtasi 1350 daraja (2460 daraja F)
Mustahkamlik chegarasi Psi – 71000 , MPa – 490
Hosildorlik (0,2%ofset) Psi – 32000 , MPa – 220
Cho'zilish 35 %

 

SS 904L EKVIVALENT baholari:

WERKSTOFF NR. 1.4539
UNS N08904
JIS SUS 904L
BS 904S13
KS STS 317J5L
AFNOR Z2 NCDU 25-20
UZ X1NiCrMoCu25-20-5

 

Jadval:

DN NPS OD(mm)
tashqi diametri
Sch5S
dyuym (mm)
Sch10S
dyuym (mm)
Sch40S
dyuym (mm)
Sch80S
dyuym (mm)
Sch160S
dyuym (mm)
6 1/8 10.3 - 0.049(1.24) 0.068(1.73) 0.095(2.41) 0.124(3.15)
8 1/4 13.7 - 0.065(1.65) 0.088(2.24) 0.119 (3.02) 0.145 (3.68)
10 3/8 17.1 - 0.065(1.65) 0.091(2.31) 0.126(3.20) 0.158(4.01)
15 1/2 21.3 0.065(1.65) 0.083(2.11) 0.109(2.77) 0.147(3.73) 0.188(4.78)
20 3/4 26.7 0.065(1.65) 0.083(2.11) 0.113(2.87) 0.154(3.91) 0.219(5.56)
25 1 33.4 0.065(1.65) 0.109(2.77) 0.133 (3.38) 0.179(4.55) 0.250(6.35)
32 1 1/4 42.2 0.065(1.65) 0.109(2.77) 0.140(3.56) 0.191(4.85) 0.250(6.35)
40 1 1/2 48.3 0.065(1.65) 0.109 (2.77) 0.145(3.68) 0.200(5.08) 0.281(7.14)
50 2 60.3 0.065(1.65) 0.109(2.77) 0.154(3.91) 0.218(5.54) 0.344(8.74)
65 2 1/2 73 0.083(2.11) 0.120(3.05) 0.203 (5.16) 0.276(7.01) 0.375(9.52)
80 3 88.9 0.083(2.11) 0.120(3.05) 0.216(5.49) 0.300(7.62) 0.438(11.13)
90 3 1/2 101.6 0.083(2.11) 0.120(3.05) 0.226(5.74) 0.318(8.08) -
100 4 114.3 0.083(2.11) 0.120(3.05) 0.237(6.02) 0.337(8.56) 0.531(13.49)
125 5 141.3 0.109(2.77) 0.134(3.40) 0.258(6.55) 0.375(9.52) 0.625(15.88)
150 6 168.3 0.109(2.77) 0.134(3.40) 0.280(7.11) 0.432(10.97) 0.719(18.26)
200 8 219.1 0.109(2.77) 0.148(3.76) 0.322(8.18) 0.500(12.70) -

 

SS 904L quvurlari ilovalari

  • Kimyoviy qayta ishlash
  • Farmatsevtika
  • Neft va gaz
  • Tuzsizlantirish

 

ASTM A312 UNS N08904 quvurlarni qadoqlash

TP904l quvurlari alohida-alohida plastik qoplarga qadoqlangan, suv o'tkazmaydigan material bilan qoplangan va neylon arqonlar bilan bog'langan. Keyin shaffof kompaniya yorlig'i 1,4547 quvur mahsuloti va miqdorini oson aniqlash uchun paketning tashqi tomoniga yopishtiriladi.

 

TSS

Savol: ASTM A312 904L zanglamaydigan po‘lat quvurlari narxlari haqidami?

Javob: Narxlar har bir kilogramm uchun 5 dan 10 dollargacha, o'lchamiga, devor qalinligiga, etkazib beruvchiga va hokazolarga qarab o'zgaradi.

Savol: Sizning yetkazib berish muddati qancha davom etadi?

Javob: Yetkazib berish muddati 5-21 kun ichida

Savol: Namuna xizmati bormi?

Javob: Namunalar bepul taqdim etiladi

Savol: Minimal buyurtma miqdori qancha?

Javob: Minimal buyurtma miqdori yo'q

Savol: Mahsulotlarni qanday qadoqlash kerak?

Javob: Ichki qatlam suv o'tkazmaydigan qog'oz tashqi qatlamiga ega va fumigatsiyali yog'och pallet bilan o'rnatiladi.

Savol: Eksport qilinadigan mamlakatlar

Javob: Braziliya, Janubiy Afrika, Indoneziya, Hindiston, Singapur, Malayziya, Eron, Rossiya, BAA, Chili, Laos va boshqalar

 

 

Issiq teglar: 904l zanglamaydigan po'lat quvur, a312 ss quvur, 904l quvur

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov