ASTM A312 zanglamaydigan po'lat quvur
video

ASTM A312 zanglamaydigan po'lat quvur


1. Standart: ASTM A312, ASME SA312
2. Turi: Choksiz, Payvandlangan
3. Hajmi: 1/2''~48''
4. Qalinligi: SCH5~SCHXXS
So'rov yuborish
Mahsulotni tanishtirish

ASTM A312 zanglamaydigan po'lat quvur choksiz, payvandlangan va og'ir sovuq ishlov berilgan ostenitik zanglamaydigan po'lat quvurlar uchun standart spetsifikatsiyadir. Yuqori harorat va umumiy korroziy xizmat ko'rsatish dasturlarida foydalanish uchun. Ushbu quvurlar yuqori quvvatga ega, mukammal korroziyaga chidamliligi, mukammal yuqori harorat ko'rsatkichlari va yaxshi ishlov berish qobiliyatiga ega.Zanglamaydigan po'lat quvur neft va gaz, neft-kimyo, oziq-ovqat mahsulotlarini qayta ishlash, farmatsevtika sanoatida keng qo'llaniladi.

 

ASTM A312 SS quvur standarti:

  • ASTM A312: Choksiz, payvandlangan va og'ir sovuq ishlov berilgan ostenitik zanglamaydigan po'lat quvurlar uchun standart spetsifikatsiya

 

  • ASTM A312 standarti ASTM A312 choksiz quvur va ASTM A312 payvandlangan quvurlarni o'z ichiga olgan har xil turdagi zanglamaydigan po'lat quvurlarni o'z ichiga oladi, 304, 304L, 316, 316L, 321, 321H, 347, 347H va boshqalar.
ASTM A312 stainless steel pipe

ASTM A312 zanglamaydigan po'lat quvurining kimyoviy tarkibi

Baho UNS C dan kichik yoki teng Mn P dan kichik yoki teng S dan kichik yoki teng Si dan kichik yoki teng Cr Mo Ni Cu
TP304 S30400 0.08 2 0.045 0.03 1 18.0-20.0 - 8.0-11.0 -
TP304L S30403 0.035 2 0.045 0.03 1 18.0-20.0 - 8.0-13.0 -
TP316 S31600 0.08 2 0.045 0.03 1 16.0-18.0 2.00-3.00 10.0-14.0 -
TP316L S31603 0.035 2 0.045 0.03 1 16.0-18.0 2.00-3.00 11.0-14.0 -
316Ti S31635 0.08 2 0.045 0.03 0.75 16.0-18.0 2.00-3.00 10.0-12.0 -
TP317 S31700 0.08 2 0.045 0.03 1 18.0-20.0 3.0-4.0 11.0-14.0 -
TP317L S31703 0.035 2 0.045 0.03 1 18.0-20.0 3.0-4.0 11.0-15.0 -
TP321 S32100 0.08 2 0.045 0.03 1 17.0-19.0 - 9.0-12.0 -
321H S32109 0.04-0.1 2 0.045 0.03 1 17.0-19.0 - 9.0-12.0 -
310 S31000 0.25 2 0.045 0.03 1.5 24.0-26.0 0.75 19.0-22.0 -
TP310S S31008 0.08 2 0.045 0.03 1 24.0-26.0 0.75 19.0-22.0 -
TP347 S34700 0.08 2 0.045 0.03 1 17.0-19.0 - 9.0-13.0 -
254SMO S31254 0.02 1 0.03 0.01 0.8 19.5-20.5 6.0-6.5 17.5-18.5 0.5-1.0
AL-6XN N08367 0.03 2 0.04 0.03 1 20.0-22.0 6.0-7.0 23.5-25.5 0.75
F904L N08904 0.02 2 0.04 0.03 1 19.0-23.0 4.0-5.0 23.0-28.0 1.0-2.0

 

ASTM A312 SS quvurining mexanik xususiyatlari

Mexanik xususiyatlar Uzilish, min, ksi[MPa】 Hosildorlik, min, ksi[MPa】 Uzayish, %(min) Qattiqlik, HB(maks)
TP304 75【515】 30【205】 35 192
TP304L 70【485】 25【170】 35 192
TP316 75【515】 30【205】 35 192
TP316L 70【485】 25【170】 35 192
316Ti 75【515】 30【205】 35 192
TP317 75【515】 30【205】 35 192
TP317L 75【515】 30【205】 35 192
TP321 75【515】 30【205】 35 192
321H 75【515】 30【205】 35 192
TP310 75【515】 30【205】 35 192
TP310S 75【515】 30【205】 35 192
TP347 75【515】 30【205】 35 192
S31254 98【675】 43【310】 35 220
N08367 100【690】 45【310】 30 241
N08926 94【650】 43【295】 35 256
N08904 71【490】 31【215】 35 192

 

Zanglamaydigan po'lat quvurning nominal o'lchamlari

DN NPS OD(mm)
tashqi diametri
Sch5S Sch10S Sch40S Sch80S Sch160S
6 1/8 10.3 - 1.24 1.73 2.41 3.15
8 1/4 13.7 - 1.65 2.24 3.02 3.68
10 3/8 17.1 - 1.65 2.31 3.2 4.01
15 1/2 21.3 1.65 2.11 2.77 3.73 4.78
20 3/4 26.7 1.65 2.11 2.87 3.91 5.56
25 1 33.4 1.65 2.77 3.38 4.55 6.35
32 1 1/4 42.2 1.65 2.77 3.56 4.85 6.35
40 1 1/2 48.3 1.65 2.77 3.68 5.08 7.14
50 2 60.3 1.65 2.77 3.91 5.54 8.74
65 2 1/2 73 2.11 3.05 5.16 7.01 9.52
80 3 88.9 2.11 3.05 5.49 7.62 11.13
90 3 1/2 101.6 2.11 3.05 5.74 8.08 -
100 4 114.3 2.11 3.05 6.02 8.56 13.49
125 5 141.3 2.77 3.40 6.55 9.53 15.88
150 6 168.3 2.77 3.40 7.11 10.97 18.26
200 8 219.1 2.77 3.76 8.18 12.7 -
250 10 273.1 3.40 4.19 9.27 12.7 -
300 12 323.9 3.96 4.57 9.53 12.7 -
350 14 355.6 3.96 4.78 9.53 12.7 -
400 16 406.4 4.19 4.78 9.53 12.7 -
450 18 457 4.19 4.78 9.53 12.7 -
500 20 508 4.78 5.54 9.53 12.7 -
550 22 559 4.78 5.54 - - -
600 24 610 5.54 6.35 9.53 12.7 -
650 26 660 - - - - -
700 28 711 - - - - -
750 30 762 6.35 7.92 - - -

 

ASTM A312 Quvur o'lchamlari bardoshlik jadvali

Standart Tashqi diametri (mm) Qalinligi (mm) Uzunlik (mm)
ASTM A312 10.29~48.26 +0.4/-0.8 +12.5/-12.5 +6.0/0
48.26~114.30 +0.8/-0.8
114.30~219.08 +1.6/-0.8
219.08~457.20 +2.4/-0.8

 

ASTM A312 quvurlarni ishlab chiqarish turlari

  • a. Choksiz quvur (SMLS): Choksiz quvur zanglamaydigan po'latdan yasalgan qattiq igna teshilishi orqali ishlab chiqariladi.
  • b. Payvandlangan quvur (WLD): payvandlash vaqtida plomba metallini qo'shmasdan avtomatik payvandlash jarayonlari (qarshilik payvandlash, elektr termoyadroviy payvandlash) tomonidan ishlab chiqarilgan payvandlangan quvurlarni o'z ichiga oladi.
  • c. Sovuq ishlov berilgan quvur (HCW trubkasi): Og'ir sovuq ishlangan quvur, har ikki devorda qalinligi kamida 35% dan kam bo'lmagan sovuq ishlov beriladi va oxirgi tavlanishdan oldin payvandlangan quvurga payvandlanadi. Payvandlash paytida plomba moddalarini ishlatmang.

 

ASTM A312 SS quvurlarini ishlab chiqarish xizmatlari

Bizning ishlab chiqarish xizmatlarimiz quyidagilarni o'z ichiga oladi: chizish va kengaytirish, issiqlik bilan ishlov berish, sovuq ishlov berish, parlatish, bükme, tavlanish va tuzlash, qum bilan ishlov berish, ishlov berish. Yetkazib beruvchilarimiz ASTM A312 choksiz quvurlarni standart ishlab chiqaruvchi sinov sertifikatlari, IBR testi, PMI testi, SGS uchinchi tomon tekshiruvi bilan ta'minlaydi.

 

ASTM A312 sinovi

  • Transvers yoki uzunlamasına valentlik sinovi
  • Yassilash testi
  • Kimyoviy tahlil
  • Mexanik sinov
  • Buzilmaydigan sinov

 

TSS

Savol: ASTM A312 zanglamas po'latdan yasalgan quvurning kg uchun narxi haqida?

Javob: Narxlar har bir kg uchun 5 dan 15 dollargacha.

Savol: Sizning yetkazib berish muddati qancha davom etadi?

Javob: Yetkazib berish muddati 5-21 kun ichida

Savol: Namuna xizmati bormi?

Javob: Namunalar bepul taqdim etiladi

Savol: Minimal buyurtma miqdori qancha?

Javob: Minimal buyurtma miqdori yo'q

Savol: Mahsulotlarni qanday qadoqlash kerak?

Javob: Ichki qatlam suv o'tkazmaydigan qog'oz tashqi qatlamiga ega va fumigatsiyali yog'och pallet bilan o'rnatiladi.

Savol: Eksport qilinadigan mamlakatlar

Javob: Braziliya, Janubiy Afrika, Indoneziya, Hindiston, Singapur, Malayziya, Eron, Rossiya, BAA, Chili, Laos va boshqalar

 

 

Issiq teglar: astm a312 zanglamaydigan po'lat quvur, a312 ss quvur, a312 quvur, zanglamaydigan po'lat quvur

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov