S304 zanglamaydigan po'lat quvur
1. Standart: ASTM A312, ASME SA312
2. Hajmi: 1/8''~30''NB
3. Qalinligi: SCH5~SCHXXS
4. End: qiyshiq uchi, tekis uchi
S304 zanglamaydigan po'lat quvurASTM A249/A312 kabi xalqaro standartlarga muvofiq ishlab chiqarilgan ostenitik zanglamaydigan po'latdan yasalgan asosiy mahsulotdir. Uning asosiy komponentlari sifatida 18% xrom va 8% nikel mavjud bo'lib, mukammal korroziyaga chidamlilik, issiqlikka chidamlilik va mexanik xususiyatlarga ega. HT PIPE - aastm a269 tp304 quvur15+ eksport tajribasiga ega yetkazib beruvchi.Biz bilan bog'lanishqo'shimcha ma'lumot va bepul takliflar uchun!
taklif qilamizS304 zanglamaydigan po'latturli shakllarda, shu jumladan:
- Bar
- Tel
- Varaq
- Plita
- Soxta buyumlar
- Quvur qismlari
- Flanjlar
- Choksiz va payvandlangan quvur
- Choksiz quvur va payvandlangan quvur
- Payvand choki

ss304 quvur asosiy mahsulot parametrlari
Material:S304 (06Cr19Ni10), Evropa Ittifoqi Idoralar, AQSh FDA va Yaponiya JIS kabi xalqaro sertifikatlash standartlariga mos keladigan material sinov hisobotlari (MTC) mavjud.
Spetsifikatsiya diapazoni:Tashqi diametri 6mm-630mm, devor qalinligi 0,8mm-20mm, moslashtirilgan uzunligi 6m, 12m yoki buyurtma bo'yicha kesiladi. Turli xil o'rnatish talablariga javob beradigan choksiz va payvandlangan turlarda mavjud.
Yuzaki ishlov berish:Pickling va passivatsiya, silliqlash (2B, BA tugatish), cho'tka bilan qoplangan. Yuzaki aniqlik mijozlar talablariga muvofiq sozlanishi, oziq-ovqat va tibbiyot sanoati kabi yuqori-standart ilovalar uchun mos keladi.
uns s30400 quvurining asosiy afzalliklari
Korroziyaga qarshilik:Atmosfera, toza suv va zaif kislota va gidroksidi muhitdan korroziyaga chidamli, oksidlanish va zangni oldini oladi. Ta'mirlash xarajatlarini kamaytiradigan tashqi ilovalar va kimyoviy suyuqliklarni tashish kabi murakkab muhitlar uchun javob beradi.
Mexanik xususiyatlari:Kuchlanish kuchi 515MPa dan katta yoki unga teng, oqish quvvati 205MPa dan katta yoki teng, mukammal egiluvchanlik, bükme, shtamplash, payvandlash va boshqa ishlov berish imkonini beradi, turli muhandislik ehtiyojlari uchun mos keladi.
Ekologik muvofiqlik:RoHS ekologik standartlariga javob beradi, zararli aralashmalarsiz va oziq-ovqat mahsulotlarini qayta ishlash, ichimlik suvi tashish va tibbiy asbob-uskunalar kabi sanitariya dasturlarida foydalanish mumkin.
S304 po'lat quvurini qo'llash
Neft va gaz:suv osti quvurlari, kislotali gaz quduqlari uchun quduq asboblari.
Kimyoviy uskunalar:sulfat kislota reaktorlari, fosfor kislotasi bug'latgichlari, tuzlash uskunalari.
Yadro sanoati:yadroviy chiqindilarni qayta ishlash tizimlari uchun konteynerlar va quvurlar.
Dengiz muhandisligi:dengiz suvini tuzsizlantirish qurilmalari, issiqlik almashinuvchilari.
Atrof-muhitni muhofaza qilish:tutun gazlarini oltingugurtdan tozalash (FGD) tizimlarining asosiy komponentlari.
ASME B36.19: S304 zanglamaydigan po'lat quvur o'lchami (in)
| Nominal quvur hajmi | OD(mm) tashqi diametri |
Sch5S (in) |
Sch10S (in) |
Sch40S (in) |
Sch80S (in) |
Sch160S (in) |
|
| DN | NPS | ||||||
| 6 | 1/8 | 10.3 | 0.049 | 0.068 | 0.095 | 0.124 | |
| 8 | 1/4 | 13.7 | 0.065 | 0.088 | 0.119 | 0.145 | |
| 10 | 3/8 | 17.1 | 0.065 | 0.091 | 0.126 | 0.158 | |
| 15 | 1/2 | 21.3 | 0.065 | 0.083 | 0.109 | 0.147 | 0.188 |
| 20 | 3/4 | 26.7 | 0.065 | 0.083 | 0.113 | 0.154 | 0.219 |
| 25 | 1 | 33.4 | 0.065 | 0.109 | 0.133 | 0.179 | 0.250 |
| 32 | 1 1/4 | 42.2 | 0.065 | 0.109 | 0.140 | 0.191 | 0.250 |
| 40 | 1 1/2 | 48.3 | 0.065 | 0.109 | 0.145 | 0.200 | 0.281 |
| 50 | 2 | 60.3 | 0.065 | 0.109 | 0.154 | 0.218 | 0.344 |
| 65 | 2 1/2 | 73 | 0.083 | 0.120 | 0.203 | 0.276 | 0.375 |
| 80 | 3 | 88.9 | 0.083 | 0.120 | 0.216 | 0.300 | 0.438 |
| 90 | 3 1/2 | 101.6 | 0.083 | 0.120 | 0.226 | 0.318 | |
| 100 | 4 | 114.3 | 0.083 | 0.120 | 0.237 | 0.337 | 0.531 |
| 125 | 5 | 141.3 | 0.109 | 0.13 | 0.258 | 0.375 | 0.625 |
| 150 | 6 | 168.3 | 0.109 | 0.13 | 0.280 | 0.432 | 0.719 |
| 200 | 8 | 219.1 | 0.109 | 0.148 | 0.322 | 0.500 | |
| 250 | 10 | 273.1 | 0.13 | 0.165 | 0.365 | 0.500 | |
| 300 | 12 | 323.9 | 0.156 | 0.18 | 0.375 | 0.500 | |
| 350 | 14 | 355.6 | 0.156 | 0.188 | 0.375 | 0.500 | |
| 400 | 16 | 406.4 | 0.165 | 0.188 | 0.375 | 0.500 | |
| 450 | 18 | 457 | 0.165 | 0.188 | 0.375 | 0.500 | |
| 500 | 20 | 508 | 0.188 | 0.218 | 0.375 | 0.500 | |
| 550 | 22 | 559 | 0.188 | 0.218 | |||
| 600 | 24 | 610 | 0.218 | 0.250 | 0.375 | 0.5 | |
| 650 | 26 | 660 | |||||
| 700 | 28 | 711 | |||||
| 750 | 30 | 762 | 0.25 | 0.312 | |||
TSS
Savol: S304 zanglamaydigan po'lat quvurlari narxlari haqida?
Javob: Narxlar kilogrammi uchun $5 - $25 dan oʻlchamiga, devor qalinligiga, yetkazib beruvchiga va hokazolarga qarab oʻzgaradi.
Savol: Sizning yetkazib berish muddati qancha davom etadi?
Javob: Yetkazib berish muddati 5-21 kun ichida
Savol: Namuna xizmati bormi?
Javob: Namunalar bepul taqdim etiladi
Savol: Minimal buyurtma miqdori qancha?
Javob: Minimal buyurtma miqdori yo'q
Savol: Mahsulotlarni qanday qadoqlash kerak?
Javob: Ichki qatlam suv o'tkazmaydigan qog'oz tashqi qatlamiga ega va fumigatsiyali yog'och sxemasidan o'rnatiladi.
Savol: Eksport qilinadigan mamlakatlar
Javob: Braziliya, Janubiy Afrika, Indoneziya, Hindiston, Singapur, Malayziya, Eron, Rossiya, BAA, Chili, Laos va boshqalar
Savol: Sizning fabrikangizga tashrif buyurishimiz mumkinmi?
Javob: Albatta, har doim xush kelibsiz!
Issiq teglar: s304 zanglamaydigan po'lat quvurlar, Xitoy s304 zanglamaydigan po'lat quvurlar ishlab chiqaruvchilari, uns s30400 quvurlari yetkazib beruvchilari
Oldingi
310MoLN quvurKeyingi2
S304 trubkasiSizga ham yoqishi mumkin
So'rov yuborish