Zanglamaydigan S316LMod trubkasi
1. Standart: ASTM A312, ASTM A213, ASTM A269
2. Hajmi: 1/8"- 48"
3. Qalinligi: 0,4 mm dan 30 mm gacha
4. Uzunlik: bitta, ikki marta tasodifiy, kesish uzunligi
Zanglamaydigan S316LMod trubkasikimyoviy tarkibi va ishlab chiqarish jarayoni yaxshilangan an'anaviy 316L ning optimallashtirilgan versiyasiga ishora qiladi. U yaxshilangan korroziyaga chidamliligi va mexanik mustahkamligi bilan ajralib turadi, og‘ir sanoat muhitiga mos keladi va -quvur loyihalari uchun tejamkor. HT PIPE - aSS 316Lmod quvuri15+ eksport tajribasiga ega yetkazib beruvchi.Biz bilan bog'lanishqo'shimcha ma'lumot va bepul takliflar uchun!
S316LMod Tube ning asosiy texnik xususiyatlari
zanglamaydigan po'latdan 316l mod Kimyoviy tarkibi
Qattiq nazorat: C 0,03% dan kam yoki teng, Mo 2,00-3,00%, Ni 13,0-15,0%, Cr 17,0-18,5%, juda kam Si va oz miqdorda N. Toʻliq ostenitik tuzilmani (ferrit) hosil qiladi.<0.5%) for better performance.
ss316lmod materiali Fizikaviy va mexanik xususiyatlari
Zichlik: 7,98 g/sm³, valentlik kuchi 485 MPa dan katta yoki unga teng, oquvchanlik 170 MPa dan katta yoki teng, cho'zilish 40% dan katta yoki unga teng, Brinell qattiqligi 217 HB dan kam yoki unga teng. 870 darajaga qadar barqarorlikni saqlaydi.
astm a312 s316lmod quvur standart va o'lcham oralig'i
ASTM A312/A213/A269, EN 10216-5, JIS G3459 bilan mos keladi. OD: 6mm-630mm, devor qalinligi: 0,4mm-30mm, choksiz / payvandlangan turlarda, har xil shakllarda va so'nggi turlarda, maxsus uzunliklarda mavjud.
Nima uchun bizni tanlaysiz?
- EN 10204/3.1B
- Xom ashyo sertifikati
- 100% rentgenografiya test hisoboti
- SGS uchinchi tomon tekshiruvi hisoboti va boshqalar
- Katta zaxira, o'z vaqtida yetkazib berish
- Bepul taklif, so'rov 24 soat ichida javob beradi

zanglamaydigan po'lat quvur 316lmod o'lchami
| Nominal quvur hajmi | OD(mm) tashqi diametri |
Sch5S (in) |
Sch10S (in) |
Sch40S (in) |
Sch80S (in) |
Sch160S (in) |
|
| DN | NPS | ||||||
| 6 | 1/8 | 10.3 | 0.049 | 0.068 | 0.095 | 0.124 | |
| 8 | 1/4 | 13.7 | 0.065 | 0.088 | 0.119 | 0.145 | |
| 10 | 3/8 | 17.1 | 0.065 | 0.091 | 0.126 | 0.158 | |
| 15 | 1/2 | 21.3 | 0.065 | 0.083 | 0.109 | 0.147 | 0.188 |
| 20 | 3/4 | 26.7 | 0.065 | 0.083 | 0.113 | 0.154 | 0.219 |
| 25 | 1 | 33.4 | 0.065 | 0.109 | 0.133 | 0.179 | 0.250 |
| 32 | 1 1/4 | 42.2 | 0.065 | 0.109 | 0.140 | 0.191 | 0.250 |
| 40 | 1 1/2 | 48.3 | 0.065 | 0.109 | 0.145 | 0.200 | 0.281 |
| 50 | 2 | 60.3 | 0.065 | 0.109 | 0.154 | 0.218 | 0.344 |
| 65 | 2 1/2 | 73 | 0.083 | 0.120 | 0.203 | 0.276 | 0.375 |
| 80 | 3 | 88.9 | 0.083 | 0.120 | 0.216 | 0.300 | 0.438 |
| 90 | 3 1/2 | 101.6 | 0.083 | 0.120 | 0.226 | 0.318 | |
| 100 | 4 | 114.3 | 0.083 | 0.120 | 0.237 | 0.337 | 0.531 |
| 125 | 5 | 141.3 | 0.109 | 0.13 | 0.258 | 0.375 | 0.625 |
| 150 | 6 | 168.3 | 0.109 | 0.13 | 0.280 | 0.432 | 0.719 |
| 200 | 8 | 219.1 | 0.109 | 0.148 | 0.322 | 0.500 | |
| 250 | 10 | 273.1 | 0.13 | 0.165 | 0.365 | 0.500 | |
| 300 | 12 | 323.9 | 0.156 | 0.18 | 0.375 | 0.500 | |
| 350 | 14 | 355.6 | 0.156 | 0.188 | 0.375 | 0.500 | |
| 400 | 16 | 406.4 | 0.165 | 0.188 | 0.375 | 0.500 | |
| 450 | 18 | 457 | 0.165 | 0.188 | 0.375 | 0.500 | |
| 500 | 20 | 508 | 0.188 | 0.218 | 0.375 | 0.500 | |
| 550 | 22 | 559 | 0.188 | 0.218 | |||
| 600 | 24 | 610 | 0.218 | 0.250 | 0.375 | 0.5 | |
| 650 | 26 | 660 | |||||
| 700 | 28 | 711 | |||||
| 750 | 30 | 762 | 0.25 | 0.312 | |||
TSS
Savol: Stainless S316LMod Tube narxlari haqida?
Javob: Narxlar kilogrammi uchun $5 - $15 dan o‘lchamiga, devor qalinligiga, yetkazib beruvchiga va hokazolarga qarab o‘zgaradi.
Savol: Sizning yetkazib berish muddati qancha davom etadi?
Javob: Yetkazib berish muddati 5-21 kun ichida
Savol: Namuna xizmati bormi?
Javob: Namunalar bepul taqdim etiladi
Savol: Minimal buyurtma miqdori qancha?
Javob: Minimal buyurtma miqdori yo'q
Savol: Mahsulotlarni qanday qadoqlash kerak?
Javob: Ichki qatlam suv o'tkazmaydigan qog'oz tashqi qatlamiga ega va fumigatsiyali yog'och sxemasidan o'rnatiladi.
Savol: Eksport qilinadigan mamlakatlar
Javob: Braziliya, Janubiy Afrika, Indoneziya, Hindiston, Singapur, Malayziya, Eron, Rossiya, BAA, Chili, Laos va boshqalar
Savol: Sizning fabrikangizga tashrif buyurishimiz mumkinmi?
Javob: Albatta, har doim xush kelibsiz!
Issiq teglar: zanglamaydigan s316lmod trubkasi, Xitoy zanglamaydigan s316lmod quvur ishlab chiqaruvchilari, ss316lmod quvurlari yetkazib beruvchilari
Oldingi
S304 trubkasiKeyingi2
ASTM A269 TP310S quvuriSizga ham yoqishi mumkin
So'rov yuborish