Asme sa 790 2205 naycha
1. Standard: AsTM A790 / ASME SA790, ASTM A928 / ASME SA928
2. Hajmi: 5. 0 - 1219. 2 mm
3. Qalinligi: {1}}. {2}} mm
4. Uzunlik: Yagona, ikki marta tasodifiy va kesilgan uzunlik
2205 (S32205,1.4462) Ikki tomonlama zanglamaydigan po'latdan yasalgan quvur ishlab chiqarish sohasida keng qo'llaniladigan yuqori samarali quvurdir. Ushbu turdagi po'lat quvurning bu turi anenit va ferritlar zanglamaydigan po'latlarning afzalliklarini birlashtiradi. Uning ajoyib mexanik xususiyatlari va korroziya qarshiligi bilan kimyo sanoati, dengiz muhandisligi, neft va gazni tashish kabi atrof-muhit uchun ideal tanlovga aylandi. HT quvuri - 15+ eksport tajribasi bo'lgan 2205 quvur etkazib beruvchi.Biz bilan bog'lanishQo'shimcha ma'lumot va narxlar bepul!
Duplex zanglamaydigan po'latdan yasalgan s31803 harorati
Uzoq muddatli foydalanish harorati 475 darajaga mo'rt fazali yoki s darajadagi mayda-bosqich yog'ingarchilik tufayli qattiqlikni kamaytirishga yo'l qo'ymaslik kerak.
Duplex Stelle 1.4462 dupleks po'latnomasi o'rtacha mos keladi
Kuchli qisqartirish kislotasida (konsentratsiya oltingugurt kislotasi) yoki yuqori konsentratsiyali gidroksozlik, korroziya qarshiligi eksperiment orqali tekshirish kerak.
F51 materialining qattiqlashuvi
Sovuq ish qilish qattiqlikning kuchayishiga olib kelishi mumkin va keyinchalik uni o'rnatish uchun yoriqlardan saqlanish uchun plastikni tiklash talab etiladi.
S31803 po'latdan yasalgan trubkani er usti davolash
Tuzlash va passivatsiya davolash asosiy plyonka plyonkasining yaxlitligini oshirishi va korroziyani uyg'otish qobiliyatini oshirishi mumkin.
Materiallarni sinovdan o'tkazish
- Qattiqlik sinovi
- Kimyoviy tahlil - spektro tahlil
- Ijobiy materialni aniqlash - PMI testi
- Test sinovi
- Mikro va makrotest
- Qarshilik testi
- Flash testi
- Intergranular korroziyasi (IGC) test

Ss 2205 quvur spetsifikatsiyasi
| Standart xususiyat |
ASTM A790 / ASME SA 790 ASTM A928 / ASME SA 928 ASTM A999 / ASME SA 999 |
| Haroratgacha (nordon muhitda) | 450 daraja F (232 daraja) |
| Ishlab chiqarish turi | Choksiz / Erv / payvandlangan / soxtalashtirilgan / CDW / CD / CDS / DOM / CEWE / 100% X rayni payvandlangan |
| Qalinlik oralig'i | Sx 5, sch10, sx 40, sch 80, sm 80s, sm 80, sm xxh, sm xs |
| Standart | SUS, Jis, Asi, AsTM, GB, EN |
| Qo'shilgan qiymat xizmatlari |
Kesish Burma Iplar Vayronagarchilik va buzg'unchilik Ultrasonik sinov Kerakli o'lchamdagi va uzunlik bo'yicha durang va kengayish |
2205 trubani qo'llash
Neft va gaz sanoati:neft quvurlari, neft va gaz quduqlari va qayta ishlash uskunalari.
Kimyo va farmatsevtika:reaktorlar, issiqlik almashuvchilar va kislota va ishqorli o'rta quvurlar.
Dengiz muhandisligi:Dengiz suvi sovutish tizimlari, o'stirish asboblari va offshor platformasi tuzilmalari.
Atrof-muhitni muhofaza qilish va energiya:Flue GasiseFeFlashtirizish (FGD) tizimlari, geotermal suyuqlik quvurlari.
Dupleks S32205 quvur oyi
| Standart | Werkstoff NR. | O'zga emas | Ro'mol |
| Dupleks S32205 | 1.4462 | S32205 | X2Crnimon 22-5-3 |
S32205 kimyoviy tarkibi
| Baho | C kamroq yoki teng | Mn kamroq yoki teng | P ga teng yoki unga teng | S dan kichik yoki unga teng | Si dan kam yoki unga teng | Ni | Kri | Mor | N | Ku |
| S32205 | 0.03 | 2 | 0.03 | 0.02 | 1 | 4.5–6.5 | 22.0–23.0 | 3.0–3.5 | 0.14–0.20 | - |
Dulex zanglamaydigan po'lat 2205 quvur mexanik xususiyatlari
| Zichlik | Eritilgan diapazon | Homiy stress (0}. 2% ofset) | Keskin stress | Cho'zish |
| 7.8 g / sm3 | 1350 daraja (2460 daraja F) | Psi - 80000, MPa - 550 | Psi - 116000, MPa - 800 | 15 % |
2205 quvurlar jadvali jadvalini (Asme B16.9)
| Dn | Nps | Od (mm) | Snacs5s (mm) ichida |
Sch10S (mm) ichida |
SCH40s (mm) ichida |
Sch80lar (mm) ichida |
Sch160s (mm) ichida |
| 6 | 1/8 | 10.3 | - | 0.049(1.24) | 0.068(1.73) | 0.095(2.41) | 0.124(3.15) |
| 8 | 1/4 | 13.7 | - | 0.065(1.65) | 0.088(2.24) | 0.119 (3.02) | 0.145 (3.68) |
| 10 | 3/8 | 17.1 | - | 0.065(1.65) | 0.091(2.31) | 0.126(3.20) | 0.158(4.01) |
| 15 | 1/2 | 21.3 | 0.065(1.65) | 0.083(2.11) | 0.109(2.77) | 0.147(3.73) | 0.188(4.78) |
| 20 | 3/4 | 26.7 | 0.065(1.65) | 0.083(2.11) | 0.113(2.87) | 0.154(3.91) | 0.219(5.56) |
| 25 | 1 | 33.4 | 0.065(1.65) | 0.109(2.77) | 0.133 (3.38) | 0.179(4.55) | 0.250(6.35) |
| 32 | 1 1/4 | 42.2 | 0.065(1.65) | 0.109(2.77) | 0.140(3.56) | 0.191(4.85) | 0.250(6.35) |
| 40 | 1 1/2 | 48.3 | 0.065(1.65) | 0.109 (2.77) | 0.145(3.68) | 0.200(5.08) | 0.281(7.14) |
| 50 | 2 | 60.3 | 0.065(1.65) | 0.109(2.77) | 0.154(3.91) | 0.218(5.54) | 0.344(8.74) |
| 65 | 2 1/2 | 73 | 0.083(2.11) | 0.120(3.05) | 0.203 (5.16) | 0.276(7.01) | 0.375(9.52) |
| 80 | 3 | 88.9 | 0.083(2.11) | 0.120(3.05) | 0.216(5.49) | 0.300(7.62) | 0.438(11.13) |
| 90 | 3 1/2 | 101.6 | 0.083(2.11) | 0.120(3.05) | 0.226(5.74) | 0.318(8.08) | - |
| 100 | 4 | 114.3 | 0.083(2.11) | 0.120(3.05) | 0.237(6.02) | 0.337(8.56) | 0.531(13.49) |
| 125 | 5 | 141.3 | 0.109(2.77) | 0.134(3.40) | 0.258(6.55) | 0.375(9.52) | 0.625(15.88) |
| 150 | 6 | 168.3 | 0.109(2.77) | 0.134(3.40) | 0.280(7.11) | 0.432(10.97) | 0.719(18.26) |
| 200 | 8 | 219.1 | 0.109(2.77) | 0.148(3.76) | 0.322(8.18) | 0.500(12.70) | - |
| 250 | 10 | 273.1 | 0.134(3.40) | 0.165(4.19) | 0.365(9.27) | 0.500(12.70) | - |
| 300 | 12 | 323.9 | 0.156(3.96) | 0.180(4.57) | 0.375(9.52) | 0.500(12.70) | - |
| 350 | 14 | 355.6 | 0.156(3.96) | 0.188(4.78) | 0.375(9.52) | 0.500(12.70) | - |
| 400 | 16 | 406.4 | 0.165(4.19) | 0.188(4.78) | 0.375(9.52) | 0.500(12.70) | - |
| 450 | 18 | 457 | 0.165(4.19) | 0.188(4.78) | 0.375(9.52) | 0.500(12.70) | - |
| 500 | 20 | 508 | 0.188(4.78) | 0.218(5.54) | 0.375(9.52) | 0.500(12.70) | - |
| 550 | 22 | 559 | 0.188(4.78) | 0.218(5.54) | - | - | - |
| 600 | 24 | 610 | 0.218(5.54) | 0.250(6.35) | 0.375(9.52) | 0.500(12.70) | - |
| 650 | 26 | 660 | - | - | - | - | - |
| 700 | 28 | 711 | - | - | - | - | - |
| 750 | 30 | 762 | 0.250(6.35) | 0.312(7.92) | - | - | - |
TSS
Savol: 2205 quvur narxi haqida?
Javob: {2 - 2 - 2 - 2 - £ 10, hajmi, devor qalinligi, etkazib beruvchi va hokazo.
Savol: Yetkazib berish muddati qancha davom etadi?
Javob: Yetkazib berish vaqti 5-21 kun ichida
Savol: namunaviy xizmat bormi?
Javob: namunalar bepul taqdim etiladi
Savol: Minimal buyurtma miqdori nima?
Javob: Minimal buyurtma miqdori yo'q
Savol: Mahsulotlarni qanday yig'ish kerak?
Javob: Ichki qatlamda suv o'tkazmaydigan qog'ozning tashqi qatlami mavjud va yog'och palet bilan o'rnatiladi.
Savol: Eksport qilingan davlatlar
Javob: Braziliya, Janubiy Afrika, Indoneziya, Indoneziya, Hindiston, Singapur, Malayziya, Eron, Rossiya, BAA, Chili, Laos va boshqalar
Savol: Sizning fabrikangizga tashrif buyurishimiz mumkinmi?
Javob: Albatta, siz doimo xush kelibsiz!
Issiq teglar: Asme sa 790 2205 truble, dupleks 1 4462 dumbline 1 4462, Super Duplex 2507 Narxi