ASTM A312 254SMO zanglamaydigan po‘lat quvur
1. Standart: ASTM A312 / ASME SA312
2. Hajmi: 1/2"- 48"
3. Qalinligi: 0.5mm-30mm
4. Ekvivalenti: UNS S31254, WNR.1.4547, AISI 254 SMO, F44
ASTM A312 254SMO zanglamaydigan po‘lat quvuryuqori darajada xrom, nikel, molibden va azotga ega bo'lgan yuqori qotishma ostenitik zanglamaydigan po'latdir. SS 254SMO quvurlari turli xil korroziy muhitlarda, shu jumladan xlorid o'z ichiga olgan muhitda chuqurchalar, yoriqlar va umumiy korroziyaga mukammal qarshilikka ega.Qotishma 254 SMOquvurlar oddiy ostenitik navlarga qaraganda kuchliroq va payvandlash osonroq. Biz choksiz va payvandlangan quvurlarni ta'minlay olamiz. Biz 15+ eksport tajribasiga ega 254SMO yetkazib beruvchimiz, biz bilan bog'laning |market@htpipe.comqo'shimcha ma'lumot va bepul takliflar uchun!
ASTM A312 254 SMO zanglamaydigan po'lat quvur standarti:
- ASTM A312: Choksiz, payvandlangan va og'ir sovuq ishlov berilgan ostenitik zanglamaydigan po'lat quvurlar uchun standart spetsifikatsiya
- Sinflar: TP304, TP304L, TP310S, TP316, TP316L, 316Ti, TP317, TP317L, TP321, TP347, TP347H, S31254, N08367, N08926 N04,
- ANSI B36.19: Zanglamaydigan po'lat quvurlar uchun spetsifikatsiya

ASTM A312 UNS S31254 zanglamaydigan po'lat quvurlarning texnik xususiyatlari
| Texnik xususiyatlari | ASTM A312 / ASME A312 |
| O'lchamlari | ASTM, ASME va API |
| O'lchamlari | 1/2" NB - 24" NB |
| Jadval | SCH5, SCH10, SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Turi | Choksiz / ERW / Payvandlangan / Tayyorlangan / LSAW quvurlari |
| Ixtisoslashgan | Katta diametrli o'lcham |
| Uzunlik | Yagona tasodifiy, ikki marta tasodifiy va kesish uzunligi. |
| Shakl | Dumaloq, kvadrat, to'rtburchaklar, gidravlik va boshqalar |
| Oxiri | To‘g‘ri uchi, qirrali uchi, pog‘onali |
A312 UNS S31254 quvurlari ekvivalent navlari
| STANDART | UNS | WERKSTOFF NR. | AFNOR | SIS | UZ |
| 254 SMO | S31254 | 1.4547 | Z1 CNDU 20.18.06Az | 2378 | X1CrNiMoCuN20-18-7 |
Qotishma 254 SMO quvurining kimyoviy tarkibi
| Baho | C | Ni | Si | N | S | Mn | P | Cr | Mo | Cu | Fe | |
| 254 SMO | min. | - | 17.5 | - | 0.18 | - | - | - | 19.5 | 6.0 | 0.5 | Balans |
| maks. | 0.02 | 18.5 | 0.08 | 0.22 | 0.01 | 1.00 | 0.03 | 20.5 | 6.5 | 1.0 | ||
SS 254 SMO quvurining mexanik xususiyatlari
| Baho | Kuchlanish kuchi (MPa) min | Cho'zilish (% 50 mm) min | Hosildorlik kuchi 0.2% Proof (MPa) min | Qattiqlik | |
| Rokvell B (HR B) maks | Brinell (HB) maks | ||||
| 254 SMO | 650 | 35 | 300 | 50 | 270 |
254smo zanglamaydigan po'lat quvurning o'lchamlari (ANSI B36.19)
| NPS (DN) | Jadval Yo'q |
Tashqi diametri, dyuym (mm) |
Devor qalinligi dyuym (mm) |
Oddiy oxiri Og'irligi (massa) Ib/ft (kg/m) |
| 1/8(6) 1/8(6) 1/8(6) 1/8(6) 1/8(6) |
5S 10S 40S 80S 160S |
0.405(10.29) 0.405(10.29) 0.405(10.29) 0.405(10.29) 0.405(10.29) |
...[Izoh(1)] 0.049(1.24)[Eslatma (1)] 0.068(1.73) 0.095(2.41) 0.124(3.15) |
... 0.19(0.28) 0.24(0.37) 0.31(0.47) 0.37(0.55) |
| 1/4(8) 1/4(8) 1/4(8) 1/4(8) 1/4(8) |
5S 10S 40S 80S 160S |
0.540(13.72) 0.540(13.72) 0.540(13.72) 0.540(13.72) 0.540(13.72) |
... [Izoh (1)] 0.065(1.65)[Eslatma(1)] 0.088(2.24) 0.119 (3.02) 0.145 (3.68) |
... 0.33(0.49) 0.43(0.63) 0.54(0.80) 0.61(0.91) |
| 3/8(10) 3/8(10) 3/8(10) 3/8(10) 3/8(10) |
5S 10S 40S 80S 160S |
0.675(17.14) 0.675(17.14) 0.675(17.14) 0.675(17.14) 0.675(17.14) |
... [Izoh(1)] 0.065(1.65)[Eslatma(1)] 0.091 (2.31) 0.126(3.20) 0.158(4.01) |
... 0.42(0.63) 0.57 (0.84) 0.74(1.10) 0.87(1.30) |
| 1/2(15) 1/2(15) 1/2(15) 1/2(15) 1/2(15) |
5S 10S 40S 80S 160S |
0.840(21.34) 0.840(21.34) 0.840(21.34) 0.840(21.34) 0.840(21.34) |
0.065(1.65)[Eslatma(1)] 0.083(2.11)[Izoh(1)] 0.109(2.77) 0.147(3.73) 0.188(4.78) |
0.54(0.80) 0.67(1.00) 0.85(1.27) 1.09(1.62) 1.31(1.95) |
| 3/4(20) 3/4(20) 3/4(20) 3/4(20) 3/4(20) |
5S 10S 40S 80S 160S |
1.050(26.67) 1.050(26.67 1.050(26.67) 1.050(26.67) 1.050(26.67) |
0.065(1.65)[Eslatma(1)] 0.083(2.11)[Izoh(1)] 0.113(2.87) 0.154(3.91) 0.219(5.56) |
0.68(1.02) 0.86(1.28) 1.13(1.68) 1.48(2.19) 1.95(2.89) |
| 1(25) 1(25) 1(25) 1(25) 1(25) |
5S 10S 40S 80S 160S |
1.315(33.40 1.315(33.40) 1.315 (33.40) 1.315(33.40) 1.315(33.40) |
0.065(1.65)[Eslatma(1)] 0.109(2.77)[Izoh(1)] 0.133 (3.38) 0.179(4.55) 0.250(6.35) |
0.87(1.29) 1.41(2.09) 1.68 (2.50) 2.17(3.24) 2.85(4.24) |
| 1 1/4 (32) 1 1/4 (32) 1 1/4 (32) 1 1/4 (32) 1 1/4 (32) |
5S 10S 40S 80S 160S |
1.660 (42.16) 1.660 (42.16) 1.660 (42.16) 1.660 (42.16) 1.660 (42.16) |
0.065(1.65)[Eslatma(1)] 0.109(2.77)[Izoh(1)] 0.140(3.56) 0.191(4.85) 0.250(6.35) |
1.11(1.65) 1.81(2.69) 2.27(3.39) 3.00 (4.46) 3.77 (5.61) |
| 1 1/2 (40) 1 1/2 (40) 1 1/2 (40) 1 1/2 (40) 1 1/2 (40) |
5S 10S 40S 80S 160S |
1.900(48.26) 1.900(48.26) 1.900(48.26) 1.900(48.26) 1.900(48.26) |
0.065(1.65)[Eslatma(1)] 0.109 (2.77)[Izoh(1)] 0.145(3.68) 0.200(5.08) 0.281(7.14) |
1.28(1.90) 2.09(3.11) 2.72 (4.05) 3.63(5.41) 4.86(7.24) |
| 2(50) 2(50) 2(50) 2(50) 2(50) |
5S 10S 40S 80S 160S |
2.375(60.32) 2.375(60.32) 2.375(60.32) 2.375(60.32) 2.375(60.32) |
0.065(1.65)[Eslatma(1)] 0.109(2.77)[Izoh(1)] 0.154(3.91) 0.218(5.54) 0.344(8.74) |
1.61(2.39) 2.64(3.93) 3.66(5.44) 5.03(7.48) 7.47(11.12) |
| 2 1/2(65) 2 1/2(65) 2 1/2(65) 2 1/2(65) 2 1/2(65) |
5S 10S 40S 80S 160S |
2.875(73.02) 2.875(73.02) 2.875(73.02) 2.875(73.02) 2.875(73.02) |
0.083(2.11)[Izoh(1)] 0.120(3.05)[Izoh(1)] 0.203 (5.16) 0.276(7.01) 0.375(9.52) |
2.48(3.69) 3.53(5.26) 5.80(8.64) 7.67(11.41) 10.02(14.91) |
| 3(80) 3(80) 3(80) 3(80) 3(80) |
5S 10S 40S 80S 160S |
3.500(88.90) 3.500(88.90) 3.500(88.90) 3.500(88.90) 3.500(88.90) |
0.083(2.11)[Izoh(1)] 0.120(3.05)[Izoh(1)] 0.216(5.49) 0.300(7.62) 0.438(11.13) |
3.03 (4.52) 4.34(6.46) 7.58(11.29) 10.26(15.27 14.34(21.35) |
| 3 1/2(90) 3 1/2(90) 3 1/2(90) 3 1/2(90) |
5S 10S 40S 80S |
4.000(101.60) 4.000(101.60) 4.000(101.60) 4.000(101.60) |
0.083(2.11)[Izoh(1)] 0.120(3.05)[Izoh(1)] 0.226(5.74) 0.318(8.08) |
3.48(5.18) 4.98 (7.41) 9.12(13.57) 12.52(18.64) |
| 4(100) 4(100) 4(100) 4(100) 4(100) |
5S 10S 40S 80S 160S |
4.500(114.30) 4.500(114.30) 4.500(114.30) 4.500(114.30) 4.500(114.30) |
0.083(2.11)[Izoh(1)] 0.120(3.05)[Izoh(1)] 0.237(6.02) 0.337(8.56) 0.531(13.49) |
3.92(5.84) 5.62(8.37) 10.80(16.08) 15.00 (22.32) 22.53(33.54) |
| 5(125) 5(125) 5(125) 5(125) 5(125) |
5S 10S 40S 80S 160S |
5.563(141.30) 5.563(141.30) 5.563(141.30) 5.563(141.30) 5.563(141.30) |
0.109(2.77)[Izoh(1)] 0.134(3.40)[Izoh(1)] 0.258(6.55) 0.375(9.52) 0.625(15.88) |
6.36(9.46) 7.78(11.56) 14.63(21.77) 20.80(30.94) 32.99(49.12) |
| 6(150) 6(150) 6(150) 6(150) 6(150) |
5S 10S 40S 80S 160S |
6.625(168.28) 6.625(168.28) 6.625(168.28) 6.625(168.28) 6.625(168.28) |
0.109(2.77)[Izoh(1)] 0.134(3.40)[Izoh(1)] 0.280(7.11) 0.432(10.97) 0.719(18.26) |
7.59(11.31) 9.30(13.83) 18.99(28.26) 28.60(42.56) 45.39 (67.56) |
| 8(200) 8(200) 8(200) 8(200) |
5S 10S 40S 80S |
8.625(219.08) 8.625(219.08) 8.625(219.08) 8.625(219.08) |
0.109(2.77)[Izoh(1)] 0.148(3.76)[Izoh(1)] 0.322(8.18) 0.500(12.70) |
9.92(14.78) 13.41(19.97) 28.58(42.55) 43.43(64.64) |
ASTM A312 UNS S31254 quvur ilovalari
- Kimyoviy qayta ishlash
- Neft va gaz
- Pulpa va qog'oz
- Tuzsizlantirish
Nima uchun bizni tanlaysiz?
- MTR (Materiallar sinovi hisoboti) EN10204
- PMI test hisobotlari
- Kimyoviy tahlil testlari
- Kuchlanish sinovlari va qattiqlik sinovlari
- Chidamlilik sinovlari
- Gidrostatik yoki buzilmaydigan elektr sinovlari
- SGS uchinchi tomon sertifikati
TSS
Savol: ASTM A312 254SMO zanglamaydigan po‘lat quvurlari narxlari haqidami?
Savol: Sizning yetkazib berish muddati qancha davom etadi?
Savol: Namuna xizmati bormi?
Savol: Minimal buyurtma miqdori qancha?
Savol: Mahsulotlarni qanday qadoqlash kerak?
Savol: Eksport qilinadigan mamlakatlar
Issiq teglar: 254smo zanglamaydigan po'lat quvur, astm a312 s31254, 254smo zanglamaydigan po'lat
Sizga ham yoqishi mumkin
So'rov yuborish