Zanglamaydigan po'latdan payvandlangan quvur
1. Turi: ASTM A312/ASME SA312, ASTM A269/ASME SA269, ASTM B676/ASME SB676
2. Hajmi: 1/2''~48''
3. Qalinligi: SCH5~SCHXXS
4. End: qiyshiq uchi, tekis uchi
Zanglamaydigan po'latdan payvandlangan quvurplitalar yoki po'lat chiziqlar chetlarini payvandlash orqali tayyorlangan po'lat quvurdir. Payvandlangan quvurlarni ishlab chiqarish jarayoni oddiy, ishlab chiqarish samaradorligi yuqori, u katta diametrli quvurlar uchun ko'proq mos keladi va narxi past, lekin umumiy quvvat choksiz po'lat quvurlarga qaraganda past. Umumiy zanglamaydigan po'lat quvurlarni payvandlash elektr qarshilik payvandlash (ERW), elektr termoyadroviy payvandlash (EFW), suv ostida payvandlash (SAW), uzunlamasına suv ostida payvandlash (SAWL) va gorizontal suv ostida payvandlash (SAWH) ni o'z ichiga oladi.
Zanglamaydigan po'latdan yasalgan payvandlangan quvur materiallari standarti:
- ASTM A312: Choksiz, payvandlangan va og'ir sovuq ishlov berilgan ostenitik zanglamaydigan po'lat quvurlar uchun standart spetsifikatsiya
- ASTM A269: Umumiy xizmat ko'rsatish uchun choksiz va payvandlangan ostenitik zanglamaydigan po'lat quvurlar uchun standart spetsifikatsiya
- ASTM B676: UNS N08367 payvandlangan quvur uchun spetsifikatsiya

Zanglamaydigan po'latdan payvandlangan quvurlarning texnik xususiyatlari
| Quvurlar texnik xususiyatlari |
ASTM A312 / ASME SA 312 ASTM A269 / ASME SA 213 ASTM B676 / ASME SB676 |
| Baho | TP304, TP304L, TP316, TP316L, 316Ti, TP317, TP317L, TP321, TP310S, TP347, S31254, N08367, N08904, 2205, 2507 va boshqalar. |
| Standart quvur | DIN, JIS, ASTM, EN, GB, AISI, ASME |
| Quvur qalinligi | 0.3mm - 50 mm |
| Payvandlangan quvur o'lchami | 5.0 mm - 1219,2 mm |
| Quvurlar jadvali | SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS |
| Quvur va quvur uchi | To'g'ri uchi, qiyshiq uchi, pog'onali quvur. |
Zanglamaydigan po'latdan payvandlangan quvurning kimyoviy tarkibi
| Baho | UNS | C dan kichik yoki teng | Mn | P dan kichik yoki teng | S dan kichik yoki teng | Si dan kichik yoki teng | Cr | Mo | Ni | Cu |
| TP304 | S30400 | 0.08 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | - | 8.0-11.0 | - |
| TP304L | S30403 | 0.035 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | - | 8.0-13.0 | - |
| TP316 | S31600 | 0.08 | 2 | 0.045 | 0.03 | 1 | 16.0-18.0 | 2.00-3.00 | 10.0-14.0 | - |
| TP316L | S31603 | 0.035 | 2 | 0.045 | 0.03 | 1 | 16.0-18.0 | 2.00-3.00 | 11.0-14.0 | - |
| 316Ti | S31635 | 0.08 | 2 | 0.045 | 0.03 | 0.75 | 16.0-18.0 | 2.00-3.00 | 10.0-12.0 | - |
| TP317 | S31700 | 0.08 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 3.0-4.0 | 11.0-14.0 | - |
| TP317L | S31703 | 0.035 | 2 | 0.045 | 0.03 | 1 | 18.0-20.0 | 3.0-4.0 | 11.0-15.0 | - |
| TP321 | S32100 | 0.08 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | - | 9.0-12.0 | - |
| 321H | S32109 | 0.04-0.1 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | - | 9.0-12.0 | - |
| 310 | S31000 | 0.25 | 2 | 0.045 | 0.03 | 1.5 | 24.0-26.0 | 0.75 | 19.0-22.0 | - |
| TP310S | S31008 | 0.08 | 2 | 0.045 | 0.03 | 1 | 24.0-26.0 | 0.75 | 19.0-22.0 | - |
| TP347 | S34700 | 0.08 | 2 | 0.045 | 0.03 | 1 | 17.0-19.0 | - | 9.0-13.0 | - |
| 254SMO | S31254 | 0.02 | 1 | 0.03 | 0.01 | 0.8 | 19.5-20.5 | 6.0-6.5 | 17.5-18.5 | 0.5-1.0 |
| AL-6XN | N08367 | 0.03 | 2 | 0.04 | 0.03 | 1 | 20.0-22.0 | 6.0-7.0 | 23.5-25.5 | 0.75 |
| F904L | N08904 | 0.02 | 2 | 0.04 | 0.03 | 1 | 19.0-23.0 | 4.0-5.0 | 23.0-28.0 | 1.0-2.0 |
Zanglamaydigan payvandlangan quvurlarning mexanik xususiyatlari
| Mexanik xususiyatlar | Uzilish, min, ksi[MPa】 | Hosildorlik, min, ksi[MPa】 | Uzayish, %(min) | Qattiqlik, HB(maks) |
| TP304 | 75【515】 | 30【205】 | 35 | 192 |
| TP304L | 70【485】 | 25【170】 | 35 | 192 |
| TP316 | 75【515】 | 30【205】 | 35 | 192 |
| TP316L | 70【485】 | 25【170】 | 35 | 192 |
| 316Ti | 75【515】 | 30【205】 | 35 | 192 |
| TP317 | 75【515】 | 30【205】 | 35 | 192 |
| TP317L | 75【515】 | 30【205】 | 35 | 192 |
| TP321 | 75【515】 | 30【205】 | 35 | 192 |
| 321H | 75【515】 | 30【205】 | 35 | 192 |
| TP310 | 75【515】 | 30【205】 | 35 | 192 |
| TP310S | 75【515】 | 30【205】 | 35 | 192 |
| TP347 | 75【515】 | 30【205】 | 35 | 192 |
| S31254 | 98【675】 | 43【310】 | 35 | 220 |
| N08367 | 100【690】 | 45【310】 | 30 | 241 |
| N08926 | 94【650】 | 43【295】 | 35 | 256 |
| N08904 | 71【490】 | 31【215】 | 35 | 192 |
SS payvandlangan quvur qo'llanilishi
Payvandlangan quvur suv, gaz, tabiiy gaz, neft, qozonxonalar, mexanik qismlar, kanalizatsiya quvurlari va boshqalar kabi katta miqdordagi suyuqlikni tashuvchi past bosimli suyuqlik quvurlari va quvurlari uchun ishlatiladi.
SS payvandlangan quvurlarni ishlab chiqarish jarayoni
Xom ashyoni yechish → tekislash → uchini kesish va payvandlash → pastadir → shakllantirish → payvandlash → ichki va tashqi payvandlash paychalarining olib tashlanishi → oldindan kalibrlash → issiqlik bilan ishlov berish → o'lchamlarni o'lchash va moslashtirish → girdob oqimini tekshirish → kesish → gidravlik bosimni tekshirish → tuzlash → yakuniy tekshirish → qadoqlash → jo‘natish.
SS payvandlangan quvur:Sifat tekshiruvi
- Transvers yoki uzunlamasına valentlik sinovi
- Yo'l bering
- Cho'zilish
- Buzilmaydigan sinov
- X-ray nuqsonlarini aniqlash
- Korroziyaga chidamlilik sinovi
- Suv bosimi sinovi
- Ultrasonik
- Yassilash testi
- Don hajmi
- Mikroskopik
- Buzilmaydigan elektr sinovlari
- Eddy oqimi
TSS
Savol: Zanglamaydigan po'latdan payvandlangan quvurlar narxlari haqida?
Savol: Sizning yetkazib berish muddati qancha davom etadi?
Savol: Namuna xizmati bormi?
Savol: Minimal buyurtma miqdori qancha?
Savol: Mahsulotlarni qanday qadoqlash kerak?
Savol: Eksport qilinadigan mamlakatlar
Issiq teglar: zanglamaydigan po'latdan payvandlangan quvur, zanglamaydigan po'lat quvur, ss payvandlangan quvur
Keyingi2
SS321 choksiz quvurSizga ham yoqishi mumkin
So'rov yuborish