316L zanglamaydigan po'lat plitalar
1. Qalinligi: 0.1mm - 50mm
2. Kengligi: 1000 - 3000 mm
3. Uzunlik: 1000 - 6000 mm
4. Ekvivalenti: UNS S31603, WNR.1.4435, WNR.1.4404, AISI 316L
316L darajasi 316 zanglamaydigan po'latdan past uglerodli variant bo'lib, molibden korroziyaga umumiy qarshilik ko'rsatadi.316L zanglamaydigan po'lat plitalar304 zanglamaydigan po'lat plitalardan yaxshiroq, bu dengiz, qirg'oq va kimyoviy muhitda qo'llanilishi uchun ko'proq mos keladi.Qotishma 316Lplitalar kislotali, gidroksidi va xlorid o'z ichiga olgan eritmalar kabi turli xil muhitlarda mukammal korroziyaga chidamliligiga ega.SS S31603shuningdek, chuqurchalar va yoriqlar korroziyasiga kuchli qarshilikka ega. Biz aSS 316L15+ eksport tajribasiga ega yetkazib beruvchi, qoʻshimcha maʼlumot va bepul narxlar uchun biz bilan bogʻlaning!
ASTM A240 tipidagi 316L zanglamaydigan po'lat plitalar standarti:
- ASTM A240: Xrom va xrom-nikel zanglamaydigan po'latdan yasalgan plitalar, varaqlar va bosimli idishlar va umumiy ilovalar uchun tasma uchun spetsifikatsiya
- Boshqa daraja: 304, 304L, 316, 316L, 316Ti, 316L Mod, 17-4ph, 310, 310S, 317, 317L, 321, 321H, 347, 347H, 904SMO5, S354L20, S32205, S31803, 2507, S31053 va boshqalar.
- Boshqa mahsulotlar: Biz taniqli ishlab chiqaruvchilar, etkazib beruvchilar va armatura, gardishlar, zarblar, mahkamlagichlar, quvurlar / quvurlar, plitalar / choyshablar / chiziqlar / rulolar, barlar / novdalar va boshqalarni eksport qiluvchimiz.

AISI 316L zanglamaydigan po'lat plitalarning texnik xususiyatlari
| Tavsif | ASTM A240 / ASME SA240 |
| Standart | ASTM, ASME, BS, DIN, EN |
| Spetsifikatsiya | Sovuq haddelenmiş: 1219mm * 2438mm (4'x8'), 1219mm * 3048mm (4'x10'), 1220mm * 2440mm, 1250mm * 2500mm yoki sizning talabingiz bo'yicha. |
| Issiq haddelenmiş: 1500mm * 2000mm, 1000mm * 3000mm, 1500mm * 4000mm, 1500m * 6000mm yoki sizning talabingiz bo'yicha. | |
| Texnika | Issiq haddelenmiş plastinka (HR), Sovuq haddelenmiş varaq (CR) |
| Yuzaki | 2B, BA, 2D, NO. 1, YO'Q. 4, NO.8, 8K, Ko‘zgu, katak, bo‘rtma, soch chizig‘i, qum portlash, cho‘tka, o‘yma |
| Qalinligi | 0.1-50 mm |
| Kengligi | 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm |
| Uzunlik | 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, 12000mm |
| Paket | Standart eksport dengiz paketi yoki kerak bo'lganda. |
| Qo'shilgan xizmatlar | Qoplama, issiqlik bilan ishlov berish, tavlangan, tuzlash, jilolash, o'rash, kesish, bükme, zarb qilish, kichik ishlab chiqarish va hk. |
316L zanglamaydigan plitalar hajmi va vazni
| Qalinligi | Qalinligi | Mavjud o'lchamlar | Og'irlik birligiga to'g'ri keladigan sirt maydoni | Har bir varaqning taxminan vazni | ||
| dyuym | mm | - | funt/ft² | kg/m² | funt | kg |
| 0.015 | 0.381 | 36 x 96 | 0.63 | 3.07566 | 15.12 | 6.84936 |
| 0.015 | 0.381 | 36 x 120 | 0.63 | 3.07566 | 18.9 | 8.5617 |
| 0.0178 | 0.45212 | 36 x 96 | 0.756 | 3.690792 | 18.15 | 8.22195 |
| 0.0178 | 0.45212 | 36 x 120 | 0.756 | 3.690792 | 22.68 | 10.27404 |
| 0.0178 | 0.45212 | 48 x 96 | 0.756 | 3.690792 | 24.19 | 10.95807 |
| 0.0178 | 0.45212 | 48 x 120 | 0.756 | 3.690792 | 30.24 | 13.69872 |
| 0.0235 | 0.5969 | 30 x 96 | 1.008 | 4.921056 | 20.16 | 9.13248 |
| 0.0235 | 0.5969 | 30 x 120 | 1.008 | 4.921056 | 25.2 | 11.4156 |
| 0.0235 | 0.5969 | 36 x 96 | 1.008 | 4.921056 | 24.19 | 10.95807 |
| 0.0235 | 0.5969 | 36 x 120 | 1.008 | 4.921056 | 30.24 | 13.69872 |
| 0.0235 | 0.5969 | 36 x 144 | 1.008 | 4.921056 | 36.29 | 16.43937 |
| 0.0235 | 0.5969 | 48 x 96 | 1.008 | 4.921056 | 32.26 | 14.61378 |
| 0.0235 | 0.5969 | 48 x 120 | 1.008 | 4.921056 | 40.32 | 18.26496 |
| 0.0235 | 0.5969 | 48 x 144 | 1.008 | 4.921056 | 48.39 | 21.92067 |
| 0.0291 | 0.73914 | 30 x 96 | 1.26 | 6.15132 | 25.2 | 11.4156 |
| 0.0291 | 0.73914 | 30 x 120 | 1.26 | 6.15132 | 31.5 | 14.2695 |
| 0.0291 | 0.73914 | 36 x 96 | 1.26 | 6.15132 | 30.24 | 13.69872 |
| 0.0291 | 0.73914 | 36 x 120 | 1.26 | 6.15132 | 37.8 | 17.1234 |
| 0.0291 | 0.73914 | 36 x 144 | 1.26 | 6.15132 | 45.37 | 20.55261 |
| 0.0291 | 0.73914 | 48 x 96 | 1.26 | 6.15132 | 40.32 | 18.26496 |
| 0.0291 | 0.73914 | 48 x 120 | 1.26 | 6.15132 | 50.41 | 22.83573 |
| 0.0291 | 0.73914 | 48 x 144 | 1.26 | 6.15132 | 60.49 | 27.40197 |
| 0.0355 | 0.9017 | 30 x 96 | 1.512 | 7.381584 | 30.24 | 13.69872 |
| 0.0355 | 0.9017 | 30 x 120 | 1.512 | 7.381584 | 37.8 | 17.1234 |
ASTM A240 tipidagi 316L SS plitasining payvandlanishi
316L zanglamaydigan po'latdan yasalgan rulonlarni payvandlash uchun oddiy payvandlash usullari, masalan, tayoqli metall boshq manbai (SMAW), gaz volfram boshq manbai (GTAW) va gazdan himoyalangan boshq manbai (GMAW) kabi payvandlash oson. Sensibilizatsiyani oldini olish va korroziyaga chidamliligini saqlab qolish uchun past issiqlik kiritish va mos plomba materiallaridan foydalanish muhimdir.
ASTM A240 TP 316L SS varaqlarini issiqlik bilan ishlov berish
Materiallar taxminan 1010 darajaga (1850 daraja F) isitiladi, ma'lum vaqt davomida ushlab turiladi va keyin tez sovutiladi, odatda suvni sovutish yoki havo sovutish orqali. Ushbu davolash materialdagi qoldiq stresslarni bartaraf etishga yordam beradi.
TSS
Savol: Bir kilogramm uchun 316L zanglamaydigan po'latdan yasalgan plitalar narxi haqida?
Savol: Sizning yetkazib berish muddati qancha davom etadi?
Savol: Namuna xizmati bormi?
Savol: Minimal buyurtma miqdori qancha?
Savol: Mahsulotlarni qanday qadoqlash kerak?
Savol: Eksport qilinadigan mamlakatlar
Issiq teglar: 316l zanglamaydigan po'lat plitalar, 316l zanglamaydigan plitalar, 316l varaqlar
Sizga ham yoqishi mumkin
So'rov yuborish