ASTM A312 TP310S zanglamaydigan po'lat quvur
1. Standart: ASTM A312 / ASME SA312
2. Hajmi: 1/8"- 30"
3. Qalinligi: SCH5~SCHXXS
4. Ekvivalenti: UNS S31008, WNR.1.4845, AISI 310S
ASTM A312 TP310S zanglamaydigan po'lat quvuruglerod, marganets, kremniy, fosfor, oltingugurt, shuningdek, xrom va nikel tarkibiga ega bo'lib, uni yuqori haroratlarda kuchli oksidlovchilarga chidamli qiladi.S31008 zanglamaydigan po'latquvur yuqori haroratlarga bardosh berishga mo'ljallangan, maksimal xizmat ko'rsatish harorati doimiy foydalanish uchun taxminan 1100 daraja (2010 daraja F) va intervalgacha foydalanish uchun taxminan 1150 daraja (2100 daraja F).1.4845 AISI 310S trubkasistandart versiyaga qaraganda kamroq uglerod tarkibiga ega, bu quvurning qattiqligini oshiradi.
ASTM A312 TP310S SS quvur standarti:
- ASTM A312: Choksiz, payvandlangan va og'ir sovuq ishlov berilgan ostenitik zanglamaydigan po'lat quvurlar uchun standart spetsifikatsiya
- Mavjud baholar: TP304, TP304L, TP316, TP316L, 316Ti, TP317, TP317L, TP310, TP310S, TP321, TP347, TP347H, S31254, N0836
- ANSI B36.19: Zanglamaydigan po'lat quvurlar uchun spetsifikatsiya

ASTM A312 TP310S zanglamaydigan po'lat quvurlari texnik xususiyatlari
| Quvurlar texnik xususiyatlari | ASTM A312 / ASME SA 312 |
| Standart quvur | DIN, JIS, ASTM, EN, GB, AISI, ASME |
| Quvur qalinligi | 0.3mm - 50 mm |
| Payvandlangan quvur hajmi | 5.0 mm - 1219,2 mm |
| Choksiz quvur tashqi diametri | 6.00 mm OD 300 mm gacha, oʻlchamlari 12” NB gacha |
| Quvurlar jadvali | SCH 5S, SCH10S, SCH 40S, SCH 80S, SCH 160S, SCH XXS, SCH XS |
| Quvur va quvur turi | Choksiz / ERW/ EFW / payvandlangan / ishlab chiqarilgan quvur |
| Quvur va quvur uchi | To'g'ri uchi, qiyshiq uchi, pog'onali quvur. |
SS 310S quvur hajmi (ASME B36.19)
| DN | NPS | OD(mm) | Sch5S (mm) |
Sch10S (mm) |
Sch40S (mm) |
Sch80S (mm) |
Sch160S (mm) |
| 6 | 1/8 | 10.3 | - | 1.24 | 1.73 | 2.41 | 3.15 |
| 8 | 1/4 | 13.7 | - | 1.65 | 2.24 | 3.02 | 3.68 |
| 10 | 3/8 | 17.1 | - | 1.65 | 2.31 | 3.2 | 4.01 |
| 15 | 1/2 | 21.3 | 1.65 | 2.11 | 2.77 | 3.73 | 4.78 |
| 20 | 3/4 | 26.7 | 1.65 | 2.11 | 2.87 | 3.91 | 5.56 |
| 25 | 1 | 33.4 | 1.65 | 2.77 | 3.38 | 4.55 | 6.35 |
| 32 | 1 1/4 | 42.2 | 1.65 | 2.77 | 3.56 | 4.85 | 6.35 |
| 40 | 1 1/2 | 48.3 | 1.65 | 2.77 | 3.68 | 5.08 | 7.14 |
| 50 | 2 | 60.3 | 1.65 | 2.77 | 3.91 | 5.54 | 8.74 |
| 65 | 2 1/2 | 73 | 2.11 | 3.05 | 5.16 | 7.01 | 9.52 |
| 80 | 3 | 88.9 | 2.11 | 3.05 | 5.49 | 7.62 | 11.13 |
| 90 | 3 1/2 | 101.6 | 2.11 | 3.05 | 5.74 | 8.08 | - |
| 100 | 4 | 114.3 | 2.11 | 3.05 | 6.02 | 8.56 | 13.49 |
| 125 | 5 | 141.3 | 2.77 | 3.40 | 6.55 | 9.53 | 15.88 |
| 150 | 6 | 168.3 | 2.77 | 3.40 | 7.11 | 10.97 | 18.26 |
| 200 | 8 | 219.1 | 2.77 | 3.76 | 8.18 | 12.7 | - |
| 250 | 10 | 273.1 | 3.40 | 4.19 | 9.27 | 12.7 | - |
| 300 | 12 | 323.9 | 3.96 | 4.57 | 9.53 | 12.7 | - |
| 350 | 14 | 355.6 | 3.96 | 4.78 | 9.53 | 12.7 | - |
| 400 | 16 | 406.4 | 4.19 | 4.78 | 9.53 | 12.7 | - |
| 450 | 18 | 457 | 4.19 | 4.78 | 9.53 | 12.7 | - |
| 500 | 20 | 508 | 4.78 | 5.54 | 9.53 | 12.7 | - |
| 550 | 22 | 559 | 4.78 | 5.54 | - | - | - |
| 600 | 24 | 610 | 5.54 | 6.35 | 9.53 | 12.7 | - |
| 650 | 26 | 660 | - | - | - | - | - |
| 700 | 28 | 711 | - | - | - | - | - |
| 750 | 30 | 762 | 6.35 | 7.92 | - | - |
SS 310S quvurining kimyoviy tarkibi
- Uglerod (C): 0, 08% maks.
- Marganets (Mn): 2.00% maks
- Fosfor (P): 0.045% maks
- Oltingugurt (S): 0.030% maks
- Kremniy (Si): 1,50% maksimal
- Chromium (Cr): 24.0-26.0%
- Nikel (Ni): 19.0-22.0%
TP310S zanglamaydigan po'lat quvur mexanik xususiyatlari
- Minimal valentlik kuchi taxminan 515 MPa (75,000 psi)
- Minimal oqish quvvati taxminan 205 MPa (30,000 psi)
- SA312 TP310S trubkasi minimal uzayishi 35%
- Maksimal qattiqlik (HB) 192
Qotishma 310S SS quvur bosimining reytingi
| Quvur hajmi (dyuym) |
Quvurlar jadvali | Harorat (F daraja) | ||||||||
| 100 | 200 | 300 | 400 | 500 | 600 | 650 | 700 | 750 | ||
| 1" | 40 | 3048 | 2629 | 2362 | 2171 | 2019 | 1924 | 1867 | 1824 | 1810 |
| 80 | 4213 | 3634 | 3265 | 3002 | 2791 | 2659 | 2580 | 2528 | 2501 | |
| 160 | 6140 | 5296 | 4759 | 4375 | 4068 | 3876 | 3761 | 3684 | 3646 | |
| 1.5" | 40 | 2257 | 1947 | 1750 | 1608 | 1496 | 1425 | 1383 | 1354 | 1340 |
| 80 | 3182 | 2744 | 2466 | 2267 | 2108 | 2009 | 1949 | 1909 | 1889 | |
| 160 | 4619 | 3984 | 3580 | 3291 | 3060 | 2916 | 2829 | 2772 | 2743 | |
| 2" | 40 | 1902 | 1640 | 1474 | 1355 | 1260 | 1201 | 1165 | 1141 | 1129 |
| 80 | 2747 | 2369 | 2129 | 1957 | 1820 | 1734 | 1682 | 1648 | 1631 | |
| 160 | 4499 | 3880 | 3486 | 3205 | 2980 | 2840 | 2755 | 2699 | 2671 | |
| 3" | 40 | 1806 | 1558 | 1400 | 1287 | 1196 | 1140 | 1106 | 1084 | 1072 |
| 80 | 2553 | 2202 | 1979 | 1819 | 1691 | 1612 | 1564 | 1532 | 1516 | |
| 160 | 3840 | 3312 | 2976 | 2736 | 2544 | 2424 | 2352 | 2304 | 2280 | |
| 4" | 40 | 1531 | 1321 | 1187 | 1091 | 1014 | 967 | 938 | 919 | 909 |
| 80 | 2213 | 1909 | 1715 | 1577 | 1466 | 1397 | 1355 | 1328 | 1314 | |
| 160 | 3601 | 3106 | 2791 | 2566 | 2386 | 2273 | 2206 | 2161 | 2138 | |
| 5" | 40 | 1342 | 1158 | 1040 | 956 | 889 | 847 | 822 | 805 | 797 |
| 80 | 1981 | 1709 | 1535 | 1411 | 1312 | 1250 | 1213 | 1189 | 1176 | |
| 160 | 3414 | 2945 | 2646 | 2433 | 2262 | 2155 | 2091 | 2049 | 2027 | |
| 6" | 40 | 1219 | 1052 | 945 | 869 | 808 | 770 | 747 | 732 | 724 |
| 80 | 1913 | 1650 | 1483 | 1363 | 1267 | 1208 | 1172 | 1148 | 1136 | |
| 160 | 3289 | 2836 | 2549 | 2343 | 2179 | 2076 | 2014 | 1973 | 1953 | |
| 8" | 40 | 1073 | 926 | 832 | 765 | 711 | 678 | 657 | 644 | 637 |
| 80 | 1692 | 1459 | 1311 | 1205 | 1121 | 1068 | 1036 | 1015 | 1005 | |
| 160 | 3175 | 2738 | 2460 | 2262 | 2103 | 2004 | 1944 | 1905 | 1885 | |
| 10" | 40 | 974 | 840 | 755 | 694 | 945 | 615 | 596 | 584 | 578 |
| 80 | 1609 | 1388 | 1247 | 1147 | 1066 | 1016 | 986 | 966 | 956 | |
| 160 | 3147 | 2714 | 2439 | 2242 | 2085 | 1986 | 1927 | 1880 | 1868 | |
ASME S ilovasiA312 310S zanglamaydigan po‘lat quvur
- neft-kimyo va kimyoviy qayta ishlash
- energiya ishlab chiqarish
- Neft va gazni qayta ishlash zavodlari
- Issiqlik almashtirgichlar va qozonlar
- Yuqori haroratli pechning tarkibiy qismlari
- Oziq-ovqat mahsulotlarini qayta ishlash uskunalari
- Farmatsevtika sanoati
TSS
Savol: ASTM A312 TP310S zanglamaydigan po'lat quvurlari narxlari haqida?
Savol: Sizning yetkazib berish muddati qancha davom etadi?
Savol: Namuna xizmati bormi?
Savol: Minimal buyurtma miqdori qancha?
Savol: Mahsulotlarni qanday qadoqlash kerak?
Savol: Eksport qilinadigan mamlakatlar
Issiq teglar: 310s zanglamaydigan po'lat quvur, a312 zanglamaydigan po'lat, 310s quvur
Sizga ham yoqishi mumkin
So'rov yuborish